    • 87. 发明申请
    • HEAT CURABLE SILICONE RUBBER COMPOSITION
    • 热固性硅橡胶组合物
    • US20150252238A1
    • 2015-09-10
    • US14438447
    • 2013-11-01
    • MOMENTIVE PERFORMANCE MATERIALS JAPAN LLC
    • Hideo TakahashiHiroyoshi IijimaHidefumi Tagai
    • C09K3/16C08L83/04
    • C09K3/16C08G77/12C08G77/20C08K5/0075C08K5/34C08K5/43C08K5/56C08L83/00C08L83/04
    • The present invention provides a heat curable silicone rubber composition capable of obtaining a cured product having a good transparency and antistatic property. A heat curable silicone rubber composition includes: (A) 100 parts by mass of an organopolysiloxane, (B) 10 to 400 parts by mass of a silicone resin, (C) an organohydrogenpolysiloxane in an amount such that the number of the hydrogen atoms bonded to a silicon atom per one alkenyl group bonded to a. silicon atom in the component (A) and the component (B) is 1.0 to 10.0, (D) a silicone rubber base polymer containing a hydrosilylation reaction catalyst, and (E) 30 to 3000 ppm of an ionic liquid serving as an antistatic agent, wherein the ionic liquid of the component (E) is one in which a difference of a refractive index from a refractive index of a cured product of the silicone rubber base polymer is within the range of ±0.04.
    • 本发明提供一种能够得到具有良好的透明性和抗静电性的固化物的热固性硅橡胶组合物。 可热固化的硅橡胶组合物包括:(A)100质量份的有机聚硅氧烷,(B)10〜400质量份的有机硅树脂,(C)有机氢聚硅氧烷,其数量使得氢原子键合数 每一个键合到一个烯基上的硅原子。 组分(A)和组分(B)中的硅原子为1.0至10.0,(D)含有氢化硅烷化反应催化剂的硅橡胶基础聚合物和(E)30至3000ppm的用作抗静电剂的离子液体 其中,组分(E)的离子液体是其中折射率与硅橡胶基础聚合物的固化产物的折射率之差在±0.04的范围内的离子液体。
    • 90. 发明授权
    • Carbon blacks-free sulfur-vulcanised electrically conductive rubber blends
    • 无炭黑硫磺化导电橡胶混合物
    • US08470210B2
    • 2013-06-25
    • US12760239
    • 2010-04-14
    • Kok Chong YongChe Su Mt Saad
    • Kok Chong YongChe Su Mt Saad
    • H01B1/12
    • H01B1/128C09K3/16
    • A practical and environmentally-friendly method, i.e. the high temperature-mechanical mixing by using an internal mixing device and a two-roll open milling device is used to produce the carbon blacks-free electrically conductive sulfur-vulcanised rubber blends of solid poly(butadiene-co-acrylonitrile) and solid sulfonic acid doped polyaniline. The addition of sulfur vulcanisation system does not affect the electrical properties of the vulcanised blends. All vulcanised blends prepared by using this method show useful electrical conductivities up to the order of 10−2 S/cm, good tensile strengths up to 18.0 MPa and colourable with the addition of a whitening agent. As a result, they have good potential to be used for manufacturing any antistatic products, electrostatic discharge or dissipative products and electromagnetic or radio frequency interferences shielding products.
    • 使用实用和环境友好的方法,即通过使用内部混合装置和双辊开放铣削装置的高温 - 机械混合来制造固体聚(丁二烯)的无炭黑导电硫硫化橡胶共混物 - 丙烯腈)和固体磺酸掺杂的聚苯胺。 加硫硫化体系不影响硫化混合物的电性能。 通过使用该方法制备的所有硫化共混物显示高达10-2S / cm的有用的电导率,高达18.0MPa的良好的拉伸强度和加入增白剂的可塑性。 因此,它们具有很好的潜力用于制造任何抗静电产品,静电放电或耗散产品以及电磁或射频干扰屏蔽产品。