    • METHOD FOR PRODUCING GRAPHITE AND PARTICULATES FOR GRAPHITE PRODUCTION
    • 生产用于石墨生产的石墨和颗粒的方法
    • US20160280549A1
    • 2016-09-29
    • US14781167
    • 2014-03-27
    • JX NIPPON OIL & ENERGY CORPORATION
    • Takashi MAEDAKunihiko SATOU
    • C01B31/04C10B57/00C10B57/04C10B55/00
    • C01B32/205C01B32/20C09C1/46C10B55/00C10B57/005C10B57/045
    • Provided are a method for producing artificial graphite through a vertical graphitization furnace with easy circulation of inert gas, uniform heating and no damage to the furnace; and particulates used therefor. The method comprises steps of: introducing graphitizable particulates having average particle diameter of 3 to 30 mm into an inside of the furnace from upper part thereof, heating the particulates at 2200° C. to 3200° C. while making inert gas flow from lower part toward upper part thereof to graphitize the particulates, and removing the graphite through lower part thereof. The particulates have average particle diameter of 3 to 30 mm and are obtained by granulating mixture comprising 100 wt parts of graphitizable carbonaceous substance powder having average particle diameter of 10 to 20 μm, 3 to 20 wt parts of binder decomposable at lower than 1000° C., and 5 to 30 wt parts of liquid which can dissolve the binder.
    • 提供一种通过垂直石墨化炉生产人造石墨的方法,其易惰性气体循环,均匀加热并且不损坏炉子; 和用于此的颗粒物。 该方法包括以下步骤:将上述平均粒径为3〜30mm的石墨化微粒从其上部引入炉内,将微粒在2200℃加热至3200℃,同时使惰性气体从下部流出 朝向其上部石墨化颗粒,并通过其下部去除石墨。 颗粒的平均粒径为3〜30mm,通过将平均粒径为10〜20μm的可石墨化碳质物质粉末100重量份,低于1000℃分解的粘合剂3〜20重量份的混合物 ,和5〜30重量份可溶解粘合剂的液体。