    • 2. 发明申请
    • METHOD FOR PREPARING HARDENED GRANULES FROM A PARTICULATE MATERIAL
    • 从颗粒材料制备硬化颗粒的方法
    • WO9717307A3
    • 1997-08-21
    • PCT/EP9604849
    • 1996-11-05
    • AECI LTDHOOGOVENS TECH SERVICESSTOTT KARL REGINALDWHITE LEROY ALANBRESLER ANDRE CHRISTIAANMAHADEW DEWANAND
    • STOTT KARL REGINALDWHITE LEROY ALANBRESLER ANDRE CHRISTIAANMAHADEW DEWANAND
    • B01J2/00B01J20/20C04B18/02C10L5/06C22B1/14C22B1/243C22B7/02C04B40/02
    • C22B7/02B01J2/00B01J20/20C04B18/021C10L5/06C22B1/14C22B1/243Y02P10/212C04B20/10
    • A method for preparing hardened granules from a particulate material which comprises admixing to the particulate material an aqueous inorganic binder, converting the resulting moist mixture into granules and hardening said granules, characterised in that it comprises the steps of: (i) selecting a particulate material comprising ingredients suitable as a raw material or an agent in a selected chemical or physical process; (ii) where applicable bringing the particulate material to a particle size distribution suitable for aggregation into granules; (iii) composing and mixing a mixture comprising: the particulate material; an aqueous inorganic binder selected from the group consisting of a calcareous binder, cementitious binder, hydraulic cement, Portland cement, high alumina cement, a mixture of a source of calciumhydroxide with a source of silica, lime, gypsum and dolomite; bringing about a moisture content so that a granulatable mixture is obtained; (iv) forming granules; (v) hardening said granules at a temperature above room temperature and below the boiling temperature of the moisture whilst sticking together of the granules is avoided and where applicable excess moisture from the granules is extracted; (vi) withdrawing the hardened granules in the form of a feed stock component for said selected process.
    • 一种从颗粒材料制备硬化颗粒的方法,其包括将水性无机粘合剂与所述颗粒材料混合,将所得湿混合物转化成颗粒并硬化所述颗粒,其特征在于其包括以下步骤:(i)选择颗粒材料 包括适合作为选择的化学或物理过程的原料或试剂的成分; (ii)如果适用,使颗粒材料达到适于聚集成颗粒的粒度分布; (iii)组合和混合包含:颗粒材料的混合物; 选自钙质粘合剂,水泥粘合剂,水硬性水泥,波特兰水泥,高铝水泥,氢氧化钙源与二氧化硅源,石灰,石膏和白云石的混合物的水性无机粘合剂; 产生含水量,从而获得可成粒的混合物; (iv)形成颗粒; (v)在高于室温且低于水分沸腾温度的温度下硬化所述颗粒,同时避免颗粒粘在一起,并且如果适用,则提取颗粒中的过量水分; (vi)以所述方法的原料成分的形式取出硬化的颗粒。