    • The strength of a compacted body is enhanced without deteriorating the magnetic properties. Additive metal powder is added to raw alloy containing a rare earth element, a transition metal element and boron to obtain a mixture, the mixture is compacted to obtain a compacted body, and the compacted body is sintered to obtain a rare earth sintered magnet. The additive metal powder is at least one species selected from the group consisting of powders of Al, Ni, Zr, Mn, Fe, Co, Cu, Zn, Ag, Sn and Bi. When adopting a process of crushing the raw alloy and a process of pulverizing the crushed raw alloy, the additive metal powder is added after the crushing process or after the pulverizing process. The amount of the additive metal powder added is 0.01 mass % or more. The additive metal powder is preferred to be platy metal alloy and, in this case, the thickness thereof is set to be 10 μm or less.
    • 增强了压实体的强度,而不会降低磁特性。 将添加金属粉末添加到含有稀土元素,过渡金属元素和硼的原料合金中,得到混合物,将其压实成压实体,将该压实体烧结,得到稀土类烧结磁体。 添加金属粉末是选自Al,Ni,Zr,Mn,Fe,Co,Cu,Zn,Ag,Sn和Bi的粉末中的至少一种。 当采用破碎原料合金的过程和粉碎的原始合金的粉碎过程时,在粉碎过程之后或粉碎过程之后添加添加金属粉末。 添加金属粉末的添加量为0.01质量%以上。 添加金属粉末优选为板状金属合金,在这种情况下,其厚度设定为10μm以下。