    • 3. 发明专利
    • CONTINUOUS CASTING COOLING METHOD FOR CONTROLLING CORNER CRACKS OF PERITECTIC STEEL SLAB
    • LU501677B1
    • 2022-09-19
    • LU501677
    • 2022-03-17
    • BAOSTEEL GROUP XINJIANG BAYI IRON AND STEEL CO LTDUNIV BEIJING SCIENCE & TECHNOLOGY
    • ZHANG CHUNHUILIU QINGWU JUNWANG HUISHENG
    • B22D11/12B21B45/02B22D11/22
    • The invention provides a continuous casting cooling method for controlling corner cracks of a peritectic steel slab, and relates to the technical field of steel continuous casting in ferrous metallurgy. Through the method, the corner cracks of the peritectic steel slab can be eliminated, other surface crack defects cannot be generated, and thus the quality of the peritectic steel continuous casting slab is effectively improved. The main contents of the method are as follows: 1) the energy-speed ratio C of a mould in the solidification process is controlled to be unchanged; 2) the ratio of the water quantity in each section of a secondary cooling zones to the total water quantity in the secondary cooling zones is as follows: a foot roller section: 27%-29%, a bending section: 35%-37%, a fan-shaped section I: 14%-15%, a fan-shaped section II: 8%-9%, and fan-shaped sections III-IV: 9%-10%; when the casting speed is less than or equal to 1.1 m/min, fan-shaped sections V-IX do not spray cooling water; when the casting speed is faster than or equal to 1.1 m/min, the spraying quantity of the fan-shaped sections V-VI is 2%-3%, and other sections do not spray cooling water; when the casting speed is faster than or equal to 1.3 m/min, the spraying quantity of the fan-shaped sections VII-IX is 2%-3%; and no spraying is performed in an area, 100 mm away from edge of the casting slab, of the fan-shaped sections. The technical scheme provided by the invention is suitable for the cooling process of steel continuous casting.