会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 8. 发明专利
    • Method for manufacturing austenitic stainless-clad steel excellent in marine corrosion resistance and low-temperature toughness
    • 在海洋耐腐蚀和低温韧性下制造奥氏体不锈钢优良的方法
    • JP2013255936A
    • 2013-12-26
    • JP2012133772
    • 2012-06-13
    • Jfe Steel CorpJfeスチール株式会社
    • KISHI KEIICHIROYAZAWA YOSHIHIROTACHIBANA SHUNICHIKURONUMA YOTAHOSHINO TOSHIYUKI
    • B21B1/38B23K20/04C21D8/02C22C38/00C22C38/38C22C38/58
    • PROBLEM TO BE SOLVED: To provide an austenitic stainless-clad steel excellent in marine corrosion resistance and low-temperature toughness.SOLUTION: In a method for manufacturing austenitic stainless-clad steel with 30 mm or more total thickness excellent in marine corrosion resistance and low-temperature toughness, a carbon steel contains, by mass%, 0.10-0.15% C; 0.25-0.40% Si; 0.45-2.0% Mn; ≤0.015% P; ≤0.004% S; ≤0.006% N; 0.01-0.1% Cr; 0.005-0.05% Nb; and 0.005-0.05% Al, and is composed of the balance Fe and unavoidable impurities, regarding the component composition. A clad steel material including the carbon steel as a base material and austenitic stainless steel as a laminated material is heated to temperature of 1,000-1,250°C before starting hot rolling, in which a cumulative rolling reduction of control rolling in a temperature range of 730-950°C is set to be 30% or more, and rolling finishing temperature is set to be 730-850°C.
    • 要解决的问题:提供优异的海洋耐腐蚀性和低温韧性的奥氏体不锈钢复合钢。解决方案:在具有30mm以上的总厚度的奥氏体不锈钢复合钢的制造方法中,耐海洋性耐腐蚀性低, - 高温韧性,碳钢以质量%计含有0.10-0.15%C; 0.25-0.40%Si; 0.45-2.0%Mn; ≤0.015%P; ≤0.004%S; ≤0.006%N; 0.01-0.1%Cr; 0.005-0.05%Nb; 和0.005-0.05%的Al,并且由组分组成的余量为Fe和不可避免的杂质构成。 将作为基材的碳素钢和作为层压材料的奥氏体不锈钢的复合钢材在起动热轧之前加热至1000〜1,250℃的温度,其中在730℃的温度范围内的控制轧制的累积压下率 -950℃设定为30%以上,轧制终轧温度设定为730〜850℃。