    • 5. 发明申请
    • PROCESS FOR PRODUCING CARBONATE COMPOUND AND CATHODE ACTIVE MATERIAL
    • 生产碳酸盐化合物和阴极活性材料的方法
    • US20150318538A1
    • 2015-11-05
    • US14798565
    • 2015-07-14
    • ASAHI GLASS COMPANY, LIMITED
    • Tomohiro SakaiTsubasa TakasugiTakuya Teratani
    • H01M4/131H01M4/505H01M10/0525C01G53/00H01M4/525
    • C01G53/006C01G53/50C01P2002/50C01P2002/52C01P2004/03C01P2004/61C01P2006/12C01P2006/40H01M4/131H01M4/505H01M4/525H01M10/0525H01M2004/028
    • To provide a carbonate compound and a cathode active material, whereby a lithium ion secondary battery having excellent cycle characteristics can be obtained.A process for producing a carbonate compound, which comprises mixing a sulfate (A) comprising a sulfate comprising a sulfate of Mn and a sulfate of Ni, or a sulfate comprising a sulfate of Mn, a sulfate of Ni and a sulfate of Co, and a carbonate (B) which is at least one carbonate selected from the group consisting of sodium carbonate and potassium carbonate, in the form of aqueous solutions and controlling the proportion of Mn to the total of Ni, Co and Mn contained in the sulfate (A) to be higher than 65 mol % at the initiation of the mixing, to precipitate a carbonate compound having a proportion of Mn of from 33.3 to 65 mol %, a proportion of Ni of from 17.5 to 50 mol % and a proportion of Co of from 0 to 33.3 mol % to the total of Ni, Co and Mn in the total average composition. A process for producing a cathode active material, which comprises mixing the carbonate compound obtained by the above process and lithium carbonate, followed by firing at from 500 to 1,000° C.
    • 为了提供碳酸盐化合物和正极活性物质,可以得到具有优异的循环特性的锂离子二次电池。 一种碳酸酯化合物的制造方法,其特征在于,将包含Mn的硫酸盐和Ni的硫酸盐的硫酸盐或含有Mn的硫酸盐的硫酸盐,Ni的硫酸盐和Co的硫酸盐组成的硫酸盐(A)和 碳酸酯(B),其为水溶液形式的至少一种选自碳酸钠和碳酸钾的碳酸盐,并控制Mn与硫酸盐中所含的Ni,Co和Mn的总量的比例(A )在混合开始时高于65mol%,使Mn的比例为33.3〜65mol%,Ni的比例为17.5〜50mol%,Co的比例为 相对于总平均组成中的Ni,Co和Mn的总和为0〜33.3摩尔%。 一种正极活性物质的制造方法,其特征在于,将上述方法得到的碳酸酯化合物与碳酸锂混合,然后在500〜1000℃下烧成。