会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 9. 发明申请
    • Dispaly screen management unit
    • 显示屏幕管理单元
    • US20070180395A1
    • 2007-08-02
    • US10582386
    • 2005-03-29
    • Ken YamashitaHidehiko Shin
    • Ken YamashitaHidehiko Shin
    • G06F3/048
    • G09G5/14G09G2320/10
    • A display screen management unit is provided which can reduce a screen resource required to switch screens and simultaneously display a pre-transition screen and a post-transition screen. When instructed to switch screens, a screen control section (103) requests a screen discard determination section (105) to determine whether or not a currently displayed screen is discarded. The screen discard determination section (105) compares currently displayed screen information with switching target screen information, and when the currently displayed screen is completely hidden by the switching target screen, determines that the currently displayed screen is discarded. The screen control section (103) discards a screen resource for the screen determined to be discarded, from a screen resource saving section (107). The screen control section (103) generates a screen resource for the switching target screen, and saves the screen resource into the screen resource saving section (107). The screen control section (103) causes a display section (106) to display the saved screen resource.
    • 提供一种显示屏管理单元,其可以减少切换屏幕所需的屏幕资源,同时显示预过渡屏幕和过渡后屏幕。 当指示切换屏幕时,屏幕控制部分(103)请求屏幕丢弃确定部分(105)确定当前显示的屏幕是否被丢弃。 屏幕丢弃确定部(105)将当前显示的画面信息与切换目标画面信息进行比较,当当前显示的画面被切换目标画面完全隐藏时,判定当前显示的画面被丢弃。 屏幕控制部(103)从画面资源保存部(107)中丢弃确定为被丢弃的画面的画面资源。 画面控制部(103)生成用于切换目标画面的画面资源,并将画面资源保存到画面资源保存部(107)。 屏幕控制部(103)使显示部(106)显示保存的画面资源。
    • 10. 发明申请
    • Weld metal excellent in low temperature toughness and SR cracking resistance used for high-strength Cr-Mo steel
    • 用于高强度Cr-Mo钢的焊接金属具有优异的低温韧性和抗SR抗裂性能
    • US20060179974A1
    • 2006-08-17
    • US11338701
    • 2006-01-25
    • Hitoshi HatanoKen Yamashita
    • Hitoshi HatanoKen Yamashita
    • C22C1/00
    • B23K35/308B23K35/3602C21D1/30
    • Disclosed is a weld metal which comprises 0.02 to 0.10% of C (% by mass; the same holds also hereinafter), 0.05 to 0.4% of Si, 0.3 to 1.3% of Mn, 0.8 to 3.25% of Cr, at most 2% (inclusive of 0%) of Mo, 0.30 to 1.0% of V, and at most 0.03% of N, wherein the contents of Al, Ti and Ni are suppressed to at most 0.03%, at most 0.03% and at most 0.40% respectively; sum total ([Mn]+[Ni]) of Mn content [Mn] and Ni content [Ni] is at most 1.2% the balance is Fe and inevitable impurities; the contents of P, S, Sn, As and Sb among the inevitable impurities are suppressed each to at most 0.01%; the content of O is suppressed to at most 0.040%; EV value as defined by related expressions satisfies EV≧0.00; and the number of carbides which have an equivalent circle diameter of at least 0.2 μm and which are present in non heat affected zone of the weld zone after being subjected to stress relieving annealing at 625° C. for 10 hours is at most 1.0 number/μm2. The weld metal, which is well suited for use in high—strength Cr—Mo steel, is improved in toughness, particularly low temperature toughness and SR cracking resistance as well, while maintaining high—temperature strength.
    • 公开了一种焊接金属,其包含C:0.02〜0.10%(质量%,以下同),Si:0.05〜0.4%,Mn:0.3〜1.3%,Cr:0.8〜3.25%,2% (包括0%)的Mo,0.30〜1.0%的V和0.03%以下的N,其中Al,Ti和Ni的含量被抑制在至多0.03%,至多0.03%和至多0.40% 分别; Mn含量[Mn]和Ni含量[Ni]的总和([Mn] + [Ni])最多为1.2%,余量为Fe和不可避免的杂质; 将不可避免的杂质中的P,S,Sn,As和Sb的含量抑制至0.01%以下。 O的含量抑制在0.040%以下; 由相关表达式定义的EV值满足EV> = 0.00; 并且在625℃下进行10分钟的应力消除退火后,存在于焊接区的非受热影响区域中具有至少0.2μm的当量圆直径的碳化物的数量为1.0个/ 妈妈<2> 。 适用于高强度Cr-Mo钢的焊接金属在保持高温强度的同时,也提高了韧性,特别是低温韧性和耐SR抗裂性。