会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 6. 发明授权
    • Pellicle frame and process for producing same
    • 防护薄膜框架及其制造方法
    • US09581897B2
    • 2017-02-28
    • US15026901
    • 2013-10-23
    • NIPPON LIGHT METAL COMPANY, LTD.
    • Takayuki YamaguchiYoshihiro Taguchi
    • G03F1/64
    • G03F1/64
    • The present invention provides a pellicle frame that can prevent generation of haze and reduces a surface glittering defect under irradiation with collected light, and a method of manufacturing the pellicle frame. Specifically, provided are a pellicle frame, including: an aluminum frame material formed of aluminum or an aluminum alloy; and an anodic oxide film on a surface of the aluminum frame material, in which the anodic oxide film includes a film formed by using an alkaline anodic oxidation solution and a film formed by using an acid anodic oxidation solution, and a method of manufacturing the pellicle frame.
    • 本发明提供一种能够防止产生雾度并减少在收集的光照射下的表面闪光缺陷的防护薄膜框架,以及制造防护薄膜框架的方法。 具体地,提供防护薄膜组件框架,其包括:由铝或铝合金形成的铝框架材料; 以及在铝框架材料的表面上的阳极氧化膜,其中阳极氧化膜包括通过使用碱性阳极氧化溶液形成的膜和使用酸性阳极氧化溶液形成的膜,以及制造防护薄膜组件的方法 帧。
    • 8. 发明申请
    • RARE EARTH ELEMENT RECOVERY METHOD
    • 稀土元素回收方法
    • US20140283652A1
    • 2014-09-25
    • US14363676
    • 2012-12-07
    • NIPPON LIGHT METAL COMPANY, LTD.
    • Kaoru SugitaYuji OtaYoshihiro TaguchiSatoshi Takeda
    • C22B59/00
    • C22B59/00B09B3/0016C22B3/0067C22B3/06C22B3/065C22B3/10Y02P10/234
    • Provided is a method of recovering rare-earth elements, including causing rare-earth elements particularly including Nd and Dy to leach efficiently from a raw material for leaching which contains the rare-earth elements, and separating and recovering the rare-earth elements. The method of recovering rare-earth elements includes: a leaching step including performing leaching treatment of rare-earth elements in which an acidic slurry of a raw material for leaching which contains the rare-earth elements is held under a predetermined condition, and then subjecting the slurry obtained after the leaching treatment to solid-liquid separation, yielding a leachate containing the rare-earth elements; and a separation step of separating and recovering the rare-earth elements from the yielded leachate, in which: the raw material for leaching contains Ca as CaO at a ratio of 4 to 15 mass % and Ti as TiO2 at a ratio of 2 to 13 mass % in a solid component (S); an acid aqueous solution is an acid aqueous solution of hydrochloric acid and/or nitric acid; and the leaching treatment performed in the leaching step is digestion or maceration which is performed under the heating and pressurizing conditions of a temperature of 160 to 300° C. and a pressure of 0.65 to 10 MPa, and the rare-earth elements are caused to leach together with Ca in the leaching step.
    • 提供一种回收稀土元素的方法,包括使特别包括Nd和Dy的稀土元素从含有稀土元素的浸出原料中有效地浸出,并分离和回收稀土元素。 回收稀土元素的方法包括:浸出步骤,包括进行稀土元素的浸出处理,其中将含有稀土元素的浸出原料的酸性浆料保持在预定条件下,然后 在浸出处理后获得的浆液进行固液分离,产生含有稀土元素的渗滤液; 以及从所得到的浸出液中分离回收稀土元素的分离工序,其中:浸出原料中含有Ca为CaO,比例为4〜15质量%,Ti为TiO 2,比例为2〜13 固体组分(S)中的质量%; 酸性水溶液是盐酸和/或硝酸的酸性水溶液; 并且在浸出步骤中进行的浸出处理是在160〜300℃的温度和0.65〜10MPa的加热加压条件下进行的消化或浸渍,并且使稀土元素 在浸出步骤中与Ca一起浸出。
    • 10. 发明申请
    • METHOD OF RECOVERING RARE-EARTH ELEMENTS
    • 恢复稀土元素的方法
    • US20150086449A1
    • 2015-03-26
    • US14389304
    • 2012-12-07
    • NIPPON LIGHT METAL COMPANY, LTD.
    • Kaoru SugitaYasushi KobayashiYoshihiro TaguchiSatoshi TakedaYuji OtaMasashi OjiriKazuhiro OdaHiroshi Sano
    • C22B59/00
    • C22B59/00B09B3/00C01F17/00C01F17/0006C22B3/0005C22B3/04C22B3/20C22B3/44C22B7/00C22B7/007Y02P10/234Y02W30/54
    • Provided is a method of recovering rare-earth elements by which rare-earth elements can be recovered efficiently from a bauxite residue serving as a raw material and containing the rare-earth elements. Specifically provided is a method of recovering rare-earth elements from a raw material, the raw material being a bauxite residue produced as a by-product in a Bayer process, the method including: using a bauxite residue having a specific surface area of 35 m2/g or more; adding, to the raw material bauxite residue, a liquid leaching agent formed of an aqueous solution of at least one kind of mineral acid selected from sulfuric acid, hydrochloric acid, nitric acid, and sulfurous acid, thereby preparing a slurry having a liquid-solid ratio of 2 to 30 and a pH of 0.5 to 2.2; subjecting the slurry to leaching treatment of the rare-earth elements under a temperature condition of room temperature to 160° C.; subjecting the slurry after the leaching treatment to solid-liquid separation, yielding a leachate; and separating and recovering the rare-earth elements from the leachate.
    • 提供一种回收稀土元素的方法,通过稀土元素可以从用作原料的铝土矿残渣中有效地回收并含有稀土元素。 具体提供的是从原料中回​​收稀土元素的方法,原料是在拜耳法中作为副产物生产的铝土矿残渣,该方法包括:使用比表面积为35m 2的铝土矿残渣 / g以上; 向原料铝土矿残渣中添加由选自硫酸,盐酸,硝酸和亚硫酸中的至少一种无机酸的水溶液形成的液体浸出剂,由此制备具有液固的浆料 比例为2至30,pH为0.5至2.2; 使该浆液在室温至160℃的温度条件下浸出处理稀土元素; 在浸出处理后对浆料进行固液分离,得到渗滤液; 并从渗滤液中分离回收稀土元素。