    • Elastomer composition and pressure-sensitive adhesive compositions
    • 弹性体组合物和压敏粘合剂组合物
    • US20060235165A1
    • 2006-10-19
    • US10544645
    • 2004-02-26
    • Takeshi KawanabeSadaharu Hashimoto
    • Takeshi KawanabeSadaharu Hashimoto
    • C08L53/02
    • C08L53/02C08L9/00C08L2666/02C09J153/02C08L2666/24
    • The invention provides an elastomer composition including an aromatic vinyl-isoprene block copolymer (a) having two or more poly(aromatic vinyl) blocks, in an amount more than 10 wt. % and less than 47.5 wt. %; an aromatic vinyl-isoprene diblock copolymer (b) in an amount more than 47.5 wt. % and less than 85 wt. %; and polyisoprene (c) having a weight average molecular weight of 20,000 to 100,000, in an amount more than 5 wt. % and less than 20 wt. %, wherein the composition has an aromatic vinyl monomer unit content more than 14 wt. % and less than 50 wt. %, based on the total amount of the components (a), (b), and (c). The elastomer composition is suitable for providing the pressure-sensitive adhesive composition, which exhibits excellent initial bond strength, peel strength, and holding power, and, even at relatively low temperature, exhibits minimal drop in initial bond strength and peel strength.
    • 本发明提供一种弹性体组合物,其包含具有两个或更多个聚(芳族乙烯基)嵌段的芳族乙烯基 - 异戊二烯嵌段共聚物(a),其量大于10wt。 %且小于47.5wt。 %; 芳族乙烯基 - 异戊二烯二嵌段共聚物(b),其量大于47.5wt。 %且小于85wt。 %; 和重均分子量为20,000至100,000的聚异戊二烯(c),其量大于5wt。 %且小于20wt。 %,其中所述组合物的芳族乙烯基单体单元含量大于14重量%。 %且小于50wt。 %,基于组分(a),(b)和(c)的总量。 弹性体组合物适用于提供初始粘合强度,剥离强度和保持力优异的粘合剂组合物,即使在相对较低的温度下,初始粘结强度和剥离强度也降低最小。
    • 2. 发明授权
    • Elastomer composition and pressure-sensitive adhesive compositions
    • 弹性体组合物和压敏粘合剂组合物
    • US07211627B2
    • 2007-05-01
    • US10544645
    • 2004-02-26
    • Takeshi KawanabeSadaharu Hashimoto
    • Takeshi KawanabeSadaharu Hashimoto
    • C08L53/02
    • C08L53/02C08L9/00C08L2666/02C09J153/02C08L2666/24
    • The invention provides an elastomer composition including an aromatic vinyl-isoprene block copolymer (a) having two or more poly(aromatic vinyl) blocks, in an amount more than 10 wt. % and less than 47.5 wt. %; an aromatic vinyl-isoprene diblock copolymer (b) in an amount more than 47.5 wt. % and less than 85 wt. %; and polyisoprene (c) having a weight average molecular weight of 20,000 to 100,000, in an amount more than 5 wt. % and less than 20 wt. %, wherein the composition has an aromatic vinyl monomer unit content more than 14 wt. % and less than 50 wt. %, based on the total amount of the components (a), (b), and (c).The elastomer composition is suitable for providing the pressure-sensitive adhesive composition, which exhibits excellent initial bond strength, peel strength, and holding power, and, even at relatively low temperature, exhibits minimal drop in initial bond strength and peel strength.
    • 本发明提供一种弹性体组合物,其包含具有两个或更多个聚(芳族乙烯基)嵌段的芳族乙烯基 - 异戊二烯嵌段共聚物(a),其量大于10wt。 %且小于47.5wt。 %; 芳族乙烯基 - 异戊二烯二嵌段共聚物(b),其量大于47.5wt。 %且小于85wt。 %; 和重均分子量为20,000至100,000的聚异戊二烯(c),其量大于5wt。 %且小于20wt。 %,其中所述组合物的芳族乙烯基单体单元含量大于14重量%。 %且小于50wt。 %,基于组分(a),(b)和(c)的总量。 弹性体组合物适用于提供初始粘合强度,剥离强度和保持力优异的粘合剂组合物,即使在相对较低的温度下,初始粘合强度和剥离强度也降低最小。
    • 3. 发明授权
    • Elastomer composition and pressure-sensitive adhesives made by using same
    • 弹性体组合物和使用它们的压敏粘合剂
    • US07674856B2
    • 2010-03-09
    • US12017965
    • 2008-01-22
    • Takeshi TaharaTakeshi Kawanabe
    • Takeshi TaharaTakeshi Kawanabe
    • C08L53/02
    • C09J153/02C08F297/04C08F297/044C08L9/00C08L53/00C08L53/02C08L2666/02C08L2666/04C08L2666/24
    • A process for the production of a pressure-sensitive adhesive composition is provided comprising (1) forming an elastomer composition by mixing in the form of a solution, 33.5 to 95% by weight of an aromatic vinyl-isoprene block copolymer (a) having two or more poly(aromatic vinyl) blocks, 0 to 47.5% by weight of an aromatic vinyl-isoprene diblock copolymer (b), and 5 to 33% by weight of isoprene homopolymer (c) having a weight average molecular weight of 20,000 to 100,000, wherein the elastomer composition has a content of aromatic vinyl monomer unit of 14 to 50% by weight, (2) separating the elastomer composition from the solvent, (3) drying the elastomer composition, and (4) blending a petroleum resin with the elastomer composition made by steps (1)-(3), wherein the amount of the petroleum resin is 10 to 500 parts by weight based on 100 parts by weight of the elastomer composition.
    • 提供一种压敏粘合剂组合物的制造方法,其包括:(1)通过以溶液的形式混合形成弹性体组合物,33.5〜95重量%的具有两个以上的芳族乙烯基 - 异戊二烯嵌段共聚物(a) 或更多的聚(芳族乙烯基)嵌段,0-47.5重量%的芳族乙烯基 - 异戊二烯二嵌段共聚物(b)和5至33重量%的重均分子量为20,000至100,000的异戊二烯均聚物(c) 其中弹性体组合物的芳族乙烯基单体单元的含量为14〜50重量%,(2)将弹性体组合物与溶剂分离,(3)干燥弹性体组合物,和(4)将石油树脂与 通过步骤(1) - (3)制备的弹性体组合物,其中基于100重量份的弹性体组合物,石油树脂的量为10-500重量份。
    • 4. 发明申请
    • Elastomer composition and pressure-sensitive adhesives made by using same
    • 弹性体组合物和使用它们的压敏粘合剂
    • US20080125545A1
    • 2008-05-29
    • US12017965
    • 2008-01-22
    • Takeshi TaharaTakeshi Kawanabe
    • Takeshi TaharaTakeshi Kawanabe
    • C08L53/02
    • C09J153/02C08F297/04C08F297/044C08L9/00C08L53/00C08L53/02C08L2666/02C08L2666/04C08L2666/24
    • A process for the production of a pressure-sensitive adhesive composition is provided comprising (1) forming an elastomer composition by mixing in the form of a solution, 33.5 to 95% by weight of an aromatic vinyl-isoprene block copolymer (a) having two or more poly(aromatic vinyl) blocks, 0 to 47.5% by weight of an aromatic vinyl-isoprene diblock copolymer (b), and 5 to 33% by weight of isoprene homopolymer (c) having a weight average molecular weight of 20,000 to 100,000, wherein the elastomer composition has a content of aromatic vinyl monomer unit of 14 to 50% by weight, (2) separating the elastomer composition from the solvent, (3) drying the elastomer composition, and (4) blending a petroleum resin with the elastomer composition made by steps (1)-(3), wherein the amount of the petroleum resin is 10 to 500 parts by weight based on 100 parts by weight of the elastomer composition.
    • 提供一种压敏粘合剂组合物的制造方法,其包括:(1)通过以溶液的形式混合形成弹性体组合物,33.5〜95重量%的具有两个以上的芳族乙烯基 - 异戊二烯嵌段共聚物(a) 或更多的聚(芳族乙烯基)嵌段,0-47.5重量%的芳族乙烯基 - 异戊二烯二嵌段共聚物(b)和5至33重量%的重均分子量为20,000至100,000的异戊二烯均聚物(c) 其中弹性体组合物的芳族乙烯基单体单元的含量为14〜50重量%,(2)将弹性体组合物与溶剂分离,(3)干燥弹性体组合物,和(4)将石油树脂与 通过步骤(1) - (3)制备的弹性体组合物,其中基于100重量份的弹性体组合物,石油树脂的量为10-500重量份。