    • Production of a Spinel Material
    • 生产尖晶石材料
    • US20150197872A1
    • 2015-07-16
    • US14420209
    • 2013-07-25
    • CSIR
    • Kenneth Ikechukwu OzoemenaCharl Jeremy Jafta
    • C30B1/04H01M4/525H01M4/505C30B30/02C30B29/22
    • C30B1/04C01G53/54C01P2002/32C01P2002/54C01P2002/72C01P2002/74C01P2002/77C01P2002/85C01P2004/03C30B29/22C30B30/02H01M4/505H01M4/525H01M2004/028
    • A process for producing a lithium-manganese-nickel oxide spinel material includes maintaining a solution comprising a dissolved lithium compound, a dissolved manganese compound, a dissolved nickel compound, a hydroxycarboxylic acid, a polyhydroxy alcohol, and, optionally, an additional metallic compound, at an elevated temperature T1, where T1 is below the boiling point of the solution, until the solution gels. The gel is maintained at an elevated temperature until it ignites and burns to form a Li—Mn—Ni—O powder. The Li—Mn—Ni—O powder is calcined to burn off carbon and/or other impurities present in the powder. The resultant calcined powder is optionally subjected 1 to microwave treatment, to obtain a treated powder, which is annealed to crystallize the powder. The resultant annealed material is optionally subjected to microwave treatment. At least one of the microwave treatments is carried out. The lithium-manganese-nickel oxide spinel material is thereby obtained.
    • 一种生产锂锰 - 氧化镍尖晶石材料的方法包括:将包含溶解的锂化合物,溶解的锰化合物,溶解的镍化合物,羟基羧酸,多羟基醇和任选的另外的金属化合物的溶液, 在高温T1,其中T1低于溶液的沸点,直到溶液凝胶化。 将凝胶保持在升高的温度,直到其点燃并燃烧形成Li-Mn-Ni-O粉末。 煅烧Li-Mn-Ni-O粉末以烧掉存在于粉末中的碳和/或其它杂质。 所得煅烧粉末任选进行1微波处理,得到经过退火处理的粉末,使粉末结晶。 任选地对所得的退火材料进行微波处理。 至少进行一次微波处理。 由此得到锂锰 - 氧化镍尖晶石材料。