会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 10. 发明申请
    • Method for Producing Inorganic Fiber-Bonded Ceramic Material
    • 生产无机纤维粘结陶瓷材料的方法
    • US20150137411A1
    • 2015-05-21
    • US14387713
    • 2013-03-21
    • Ube Industries, Ltd.
    • Kenji MatsunagaShinji KajiiShohei SuizuTsutomu Kodama
    • C04B35/645C04B35/10
    • C04B35/645B29C43/10B29C43/14B29C2043/106B29C2043/3205B32B18/00C04B35/10C04B35/593C04B35/6268C04B35/62849C04B35/62897C04B35/80C04B2235/524C04B2235/5244C04B2235/5256C04B2235/5264C04B2235/6587C04B2235/661C04B2235/96C04B2237/38C04B2237/70
    • Provided is a method for producing an inorganic fiber-bonded ceramic material, which can produce, at a high yield, an inorganic fiber-bonded ceramic material with fewer defects, and with an end part and a central part equivalent to each other in microstructure and mechanical properties, and also makes it possible to increase the ceramic material in size. The method for producing an inorganic fiber-bonded ceramic material is characterized in that it includes: a first pressing step of setting, in a carbon die, a laminate to be surrounded by a ceramic powder, the laminate obtained by stacking a coated inorganic fiber shaped product including an inorganic fiber part of inorganic fibers that have a pyrolysis initiation temperature of 1900° C. or lower, and a surface layer of an inorganic substance for bonding the inorganic fibers to each other, and pressing the laminate at a temperature of 1000 to 1800° C. and a pressure of 5 to 50 MPa in an inert gas atmosphere; and a second pressing step of pressing a ceramic coated laminate obtained in the first pressing step at a temperature of 1600 to 1900° C., which is higher than that in the first pressing step, and at a pressure of 5 to 100 MPa in an inert gas atmosphere.
    • 本发明提供一种无机纤维结合陶瓷材料的制造方法,其能够以高收率生产缺陷少的无机纤维结合陶瓷材料,并且在微观结构和相互之间具有彼此相当的端部和中心部分 机械性能,并且还可以增加陶瓷材料的尺寸。 无机纤维结合陶瓷材料的制造方法的特征在于,包括:第一加压工序,在碳纤维模具中设置被陶瓷粉末包围的层叠体,将通过层叠被覆无机纤维状 包括热解开始温度为1900℃以下的无机纤维的无机纤维部分和将无机纤维彼此粘合的无机物质的表面层,在1000℃以上的温度下压制层压体 1800℃,压力为5〜50MPa; 以及第二压制步骤,在第一压制步骤中获得的陶瓷涂覆层压板在1600至1900℃的温度下压制,其温度高于第一压制步骤,并且在5-100MPa的压力下, 惰性气体气氛。