    • Method for the continuous sintering of mineral material and sintering equipment
    • 矿物材料和烧结设备的连续烧结方法
    • US09534844B2
    • 2017-01-03
    • US13813622
    • 2011-09-21
    • Päivi Oikarinen
    • Päivi Oikarinen
    • F27B9/00F27B21/00C22B1/20C22B1/26F27B21/06F27D7/02F27B9/30F27D9/00
    • F27B21/00C22B1/205C22B1/26F27B9/30F27B21/06F27D7/02F27D9/00
    • The invention relates to a method and equipment for the continuous sintering of mineral material in a sintering furnace (S). In the method, a material bed (2) is formed on a conveyor base (1), the material bed (2) is conveyed by the conveyor base (1) through the process zones (I-VII) of the sintering furnace that have different temperatures, the zones including at least one drying zone (I), at least one cooling zone (VII), and at least one other process zone (II, III, IV, V, VI) between the said drying zone and cooling zone, and gas is conducted through the conveyor base and the material bed (2), when the material bed travels through the process zones (I-VII), and gas is circulated in a circulation gas duct (3) from the last cooling zone (VII) to the drying zone (I). Part of the gas flow that is conducted to the drying zone (I) in the circulation gas duct (3) is removed as an exhaust gas flow (B) by the exhaust gas blower (5) of an exhaust gas duct (4). The volume flow of the exhaust gas flow (B) is regulated by regulating the blowing power of the blower (5) to control the temperature of the gas flow travelling through the material bed in the drying zone.
    • 本发明涉及烧结炉(S)中矿物材料的连续烧结的方法和设备。 在该方法中,在输送机基座(1)上形成材料床(2),料床(2)由输送机基座(1)通过烧结炉的加工区(I-VII)输送, 所述区域包括在所述干燥区域和冷却区域之间的至少一个干燥区域(I),至少一个冷却区域(VII)和至少一个其它处理区域(II,III,IV,V,VI) 当材料床通过处理区域(I-VII)时,气体通过输送机基座和材料床(2)传导,并且气体在循环气体管道(3)中从最后一个冷却区域循环( VII)至干燥区(I)。 通过废气导管(4)的排气鼓风机(5)将作为排气流(B)排出到循环气体管道(3)中的干燥区域(I)的一部分气流被除去。 通过调节鼓风机(5)的吹送功率来控制排气流(B)的体积流量,以控制在干燥区中通过材料床行进的气流的温度。
    • 8. 发明授权
    • Process for sintering on a sintering machine
    • 烧结机烧结工艺
    • US07914731B2
    • 2011-03-29
    • US12161205
    • 2007-01-12
    • Karl LaaberOskar PammerHans-Herbert StiasnyAnton SebanzKarl Zehetbauer
    • Karl LaaberOskar PammerHans-Herbert StiasnyAnton SebanzKarl Zehetbauer
    • C22B1/20
    • C22B1/20C22B1/205F27B21/06
    • A process for sintering metal-containing materials, such as iron ores or manganese ores, on a sintering machine including a sintering belt for transporting the sinter mix during sintering thereof. The sintering belt has first, second and third portions. Sintering waste gas from the third portion is transported to and unified with sintering waste gas from the first portion in a mixing region to form a mixed gas, wherein the transporting distance of the sintering waste gas from the third portion to the mixing region is greater than the transporting distance of the sintering waste gas from the first portion to the mixing region. An apparatus for carrying out the process is disclosed, including the sintering belt, suction boxes operative at the portions of the belt, and lines for conveying the gas produced and the gases used in the process.
    • 一种在包含用于在其烧结期间输送烧结混合物的烧结带的烧结机上烧结含金属材料如铁矿石或锰矿石的方法。 烧结带具有第一,第二和第三部分。 来自第三部分的烧结废气被输送到混合区中的来自第一部分的烧结废气并形成混合气体,其中烧结废气从第三部分到混合区的输送距离大于 烧结废气从第一部分到混合区域的输送距离。 公开了一种用于执行该方法的装置,包括烧结带,在带的部分操作的抽吸箱和用于输送所产生的气体和用于该过程的气体的管线。
    • 9. 发明申请
    • Process for producing sintering feedstock and apparatus therefor
    • 生产烧结原料的方法及其设备
    • US20050050995A1
    • 2005-03-10
    • US10497304
    • 2003-03-28
    • Nobuyuki OyamaKanji AizawaTakayuki Ueki
    • Nobuyuki OyamaKanji AizawaTakayuki Ueki
    • C22B1/20C22B1/243C22B1/00
    • C22B1/20C22B1/243
    • A simple and economical manufacturing method of a sintering material for manufacturing a sintering material suitable for manufacturing sintered ore excellent in the reducibility and high in the cold strength, and an apparatus therefor are proposed. As a pretreatment of a manufacturing process of sintered ore for use in a blast furnace by use of a Dwight-Lloyd type sintering machine of downward suction, a sintering material including iron ore, a SiO2-containing material, a limestone base powdery material and a solid fuel type powdery material is projected as a additional coating auxiliary raw material into the drum mixer with a additional coating conveyor disposed in proximity to an exhaust outlet of the drum mixer. Preferably, a sintering material excepting a limestone base powdery material and a solid fuel type powdery material is charged from a charge inlet of the drum mixer to granulate and in a region disposed in the middle on a downstream side where a staying time during which the sintering material reaches an exhaust outlet of the drum mixer is in the range of from 10 to 90 seconds, a additional coating auxiliary raw material including a limestone base powdery material and a solid fuel type powdery material is added, and thereby until reaching the exhaust outlet, the additional coating auxiliary raw material is deposited and formed on a exterior coating portion of the sintering material.
    • 提出了一种用于制造适合于制造具有优异的还原性和高的冷却强度的烧结矿的烧结材料的烧结材料的简单且经济的制造方法及其装置。 作为用于高炉的烧结矿的制造方法的预处理,使用德怀特 - 劳埃德式的向下吸入式烧结机,可以使用包含铁矿石,含SiO 2的材料,石灰石基础粉末材料和 将固体燃料型粉末材料作为另外的涂层辅助原料投影到鼓式混合器中,附加涂层输送器设置在鼓式混合器的排气出口附近。 优选地,除了石灰石基础粉末材料和固体燃料型粉末材料之外的烧结材料从鼓式混合机的充电入口装入颗粒,并且在设置在中间的区域中,在下游侧具有烧结 材料到达鼓式搅拌机的排气出口在10〜90秒的范围内,添加包括石灰石粉末材料和固体燃料型粉末材料的附加涂层辅助原料,从而直到到达排气出口, 附加的涂层辅助原料沉积并形成在烧结材料的外涂层部分上。