    • 34. 发明授权
    • Process of producing thermoplastic polymer blends
    • 生产热塑性聚合物共混物的方法
    • US07919561B2
    • 2011-04-05
    • US11446794
    • 2006-06-05
    • Terry J. BurkhardtAspy K. Mehta
    • Terry J. BurkhardtAspy K. Mehta
    • C08L23/00C08L23/04C08F8/00C08F210/00
    • C08L23/12C08L23/10C08L23/14C08L23/142C08L2205/02C08L2666/06
    • A process is described for producing a polymer blend comprising (a) a first polymer component comprising a crystalline propylene polymer and (b) a second polymer component comprising a copolymer of propylene with at least one comonomer, wherein the copolymer comprises between about 7 wt % and about 28 wt % of comonomer and the copolymer has a heat of fusion of 0.5 to 70 J/g and an mm triad tacticity of 75% or greater. The process comprises polymerizing propylene under first polymerization conditions in a polymerization reaction zone to produce a first effluent comprising a crystalline propylene polymer containing no more than 10% by weight of other monomers, the first polymerization conditions comprising a first reaction temperature between about 50° C. and about 100° C. Propylene is then copolymerized with at least one comonomer under second polymerization conditions in the presence of a metallocene catalyst and at least part of said first effluent in a slurry polymerization reaction zone to produce the second polymer component as a blend with the first polymer component, the second polymerization conditions comprising a second reaction temperature at least 7° C. less than the first reaction temperature.
    • 描述了一种制备聚合物共混物的方法,其包含(a)包含结晶丙烯聚合物的第一聚合物组分和(b)包含丙烯与至少一种共聚单体的共聚物的第二聚合物组分,其中所述共聚物包含约7重量% 和约28重量%的共聚单体,共聚物的熔融热为0.5〜70J / g,mm三元组立构规整度为75%以上。 该方法包括在聚合反应区中在第一聚合条件下聚合丙烯以产生包含不超过10重量%的其它单体的结晶丙烯聚合物的第一流出物,第一聚合条件包括约50℃的第一反应温度 然后约100℃。然后,丙烯在第二聚合条件下,在茂金属催化剂和至少部分所述第一流出物在淤浆聚合反应区中的存在下,与至少一种共聚单体共聚以产生作为共混物的第二聚合物组分 与第一聚合物组分相比,第二聚合条件包括比第一反应温度低至少7℃的第二反应温度。
    • 37. 发明授权
    • Homogeneous polymer blend and articles therefrom
    • 均相聚合物共混物及其制品
    • US07619038B2
    • 2009-11-17
    • US11299022
    • 2005-12-09
    • Aspy K. MehtaChia ChengSudhin DattaWen LiChon Y. LinSrivatsan S. Iyer
    • Aspy K. MehtaChia ChengSudhin DattaWen LiChon Y. LinSrivatsan S. Iyer
    • C08L23/10C08L23/14
    • C08L23/10C08L23/142C08L2205/02C08L2205/025C08L2314/06C08L2666/06
    • This invention relates to homogeneous blends of: 1) from 60 to 99 weight percent of one or more semi-crystalline polymers (based upon the weight of the semi-crystalline and semi-amorphous polymers), each semi-crystalline polymer comprising propylene and from 0 to 5 weight % alpha-olefin comonomer (based upon the weight of the polymer), said semi-crystalline polymers each having a melting point between 100 and 170° C. and a melt flow rate of 200 dg/min or less; and 2) from 1 to 40 weight % of one or more semi-amorphous polymers (based upon the weight of the semi-crystalline and semi-amorphous polymers), each semi-amorphous polymer comprising propylene and from 5 to 12 weight % of one or more C2 and or C4 to C10 alpha-olefin comonomers, said semi-amorphous polymers each having: a) 10 to 50 percent crystallinity or less; b) a melt flow rate of 200 dg/min or less; c) a DSC melting point (second melt Tm) of 130° C. or less; d) an intermolecular composition distribution as determined by thermal fractionation in hexane such that 85% by weight or more of the polymer is isolated as one or two adjacent, soluble fractions with the balance of the polymer in immediately preceding or succeeding fractions; and wherein each of these fractions has a wt % comonomer content with a difference of no greater than 20 wt % relative to the average wt % comonomer content of the copolymer; e) an Mw/Mn of 1.5 to 4, f) a triad tacticity of three propylene units, as measured by 13C NMR, of 75% or greater, for use in films, fibers, non-wovens, molded articles and the like.
    • 本发明涉及以下均质共混物:1)60至99重量%的一种或多种半结晶聚合物(基于半结晶和半无定形聚合物的重量),每种半结晶聚合物包含丙烯和 0至5重量%的α-烯烃共聚单体(基于聚合物的重量),所述半结晶聚合物各自具有100-170℃的熔点和200dg / min以下的熔体流动速率; 和2)1至40重量%的一种或多种半无定形聚合物(基于半结晶和半无定形聚合物的重量),每种包含丙烯的半无定形聚合物和5至12重量%的一种 或更多的C 2和C 4至C 10α-烯烃共聚单体,所述半无定形聚合物各自具有:a)10至50%的结晶度或更低; b)200dg / min或更低的熔体流动速率; c)130℃或更低的DSC熔点(第二熔体Tm); d)通过在己烷中的热分馏测定的分子间组成分布,使得85重量%或更多的聚合物作为一个或两个相邻的可溶性级分分离,在紧邻的前面或后续级分中余量的聚合物分离; 并且其中这些级分中的每一种都具有相对于共聚物的平均重量%共聚单体含量的不大于20重量%的重量%共聚单体含量; e)Mw / Mn为1.5至4,f)通过13 C NMR测量的三个丙烯单元的三单元组立构规整度为75%或更大,用于膜,纤维,无纺布,模制品等。