    • Pipe Comprising a Metallocene-Catalyzed Polyethylene Resin
    • 包含茂金属催化聚乙烯树脂的管道
    • US20170058063A1
    • 2017-03-02
    • US15305683
    • 2015-04-23
    • Total Research & Technology Feluy
    • Olivier LhostJacques Michel
    • C08F210/16F16L9/127
    • C08F210/16C08F10/02C08F110/02C08F210/02C08F2500/05C08L2205/025C08L2308/00C08L2314/06F16L9/127C08F2/001C08F4/65927C08F210/14C08F2500/12
    • The invention relates to a pipe comprising at least one metallocene-catalyzed polyethylene resin, wherein the polyethylene resin has a multimodal molecular weight distribution and comprises at least two metallocene-catalyzed polyethylene fractions A and B, wherein fractions A and B are prepared in different reactors of at least two reactors connected in series, wherein the polyethylene resin comprises: at least 30% by weight and at most 50% by weight of the polyethylene fraction A, based on the total weight of the polyethylene resin, wherein fraction A has a melt index MI2 of at least 50 g/10 min as determined on the fluff of fraction A according to ISO 1133:1997 condition D at a temperature of 190° C. and under a load of 2.16 kg; wherein fraction B has a density of at most 0.9210 g/cm3; and wherein the polyethylene resin has a melt index MI5 of at least 0.10 g/10 min and of at most 1.0 g/10 min as determined according to ISO 1133:1997, condition T, at 190° C. and under a load of 5 kg; wherein the polyethylene resin has an HLMI of at least 4.0 g/10 min and at most 14.0 g/10 min, as measured according to the procedure of ISO 1133:1997 condition G with a temperature of 190° C. and a load of 21.6 kg; and a density of at least 0.9420 g/cm3 and of at most 0.9460 g/cm3 as determined according to the procedure of ASTM D-1505 at a temperature of 23° C.
    • 本发明涉及包含至少一种茂金属催化的聚乙烯树脂的管,其中聚乙烯树脂具有多峰分子量分布并且包含至少两种茂金属催化的聚乙烯级分A和B,其中级分A和B在不同的反应器 的至少两个反应器串联连接,其中所述聚乙烯树脂包含:聚乙烯部分A的至少30重量%和至多50重量%,基于聚乙烯树脂的总重量,其中部分A具有熔体 根据ISO 1133:1997条件D在190℃的温度和2.16kg的负荷下,根据分数A的绒毛测定的至少50g / 10min的指数M12为至少50g / 10min; 其中级分B具有至多0.9210g / cm 3的密度; 并且其中所述聚乙烯树脂的熔体指数M15为至少0.10g / 10min且至多1.0g / 10min,根据ISO1 133:1997,条件T在190℃和5kg负载下测定; 其中所述聚乙烯树脂的HLMI为至少4.0g / 10min且至多14.0g / 10min,根据ISO1133:1997的条件G测量,温度为190℃,负荷为21.6kg; 并且根据ASTM D-1505的程序在23℃的温度下测定的密度为至少0.9420g / cm 3且至多0.9460g / cm 3。