会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 1. 发明授权
    • Construction built from waste tires and its constructing method
    • 废轮胎施工及其施工方法
    • US07137758B2
    • 2006-11-21
    • US11030765
    • 2005-01-07
    • Ming-Hui Chou
    • Ming-Hui Chou
    • E02D29/02
    • E02B3/046E02B2201/04E02D17/20Y02W30/687Y10S52/09
    • A constructing method by using waste tires includes cutting sidewalls from waste tires; connecting multiple waste tires in series together by the sidewalls to form a layer of waste tires; filling the waste tires with ballast; and stacking another layer of waste tires on the previous layer with a staggered arrangement. An end member, being composed of a cut waste tire with two ends connected to an outer periphery of an unbroken waste tire, is provided at an end portion of the layers. Whereby, the construction built from waste tires can be used in projects such as a protection slope, road berm, riverbank, riverbed, etc., and has a good strength and a low cost.
    • 使用废轮胎的构造方法包括从废轮胎切割侧壁; 通过侧壁将多个废轮胎串联在一起以形成一层废轮胎; 用压载物填充废轮胎; 并以交错布置在另一层上堆叠另一层废轮胎。 在各层的端部设置有端部构件,其由具有连接到不间断的废轮胎的外周的两端的切断废轮构成。 由废轮胎建造的建筑物可用于保护坡道,道路护堤,河岸,河床等工程,具有较强的实力和较低的成本。
    • 3. 发明授权
    • Method to produce an anti-swelling mica
    • 产生抗肿胀云母的方法
    • US07232481B1
    • 2007-06-19
    • US11416776
    • 2006-05-03
    • Ming-Hui Chou
    • Ming-Hui Chou
    • C04B14/20C01B33/26
    • C01B33/42C04B14/206
    • A method to produce an anti-swelling mica having following steps: mixing powdery mica with an alkaline compound to form a mixture; heating the mixture at a temperature between 150° C.˜230° C. for lasting 30 minutes to make metal ions out of the alkaline compound to diffuse into the mica homogeneously; using water to reduce temperature of the mixture so as to form an alkaline solution; separating the powdery mica from the alkaline solution to obtain a solid mica; neutralizing excessive alkaline compound adhering to the solid mica by an acid solution that is diluted by cold water and the mica anti-swells after adjusting pH of the solid mica to less than 7.0; and diluting the acid solution again by adding water and separating the solid mica from diluted acid solution to obtain a production—anti-swelling mica.
    • 一种生产抗肿胀云母的方法,具有以下步骤:将粉状云母与碱性化合物混合以形成混合物; 在150℃〜230℃的温度下加热混合物持续30分钟,使金属离子从碱性化合物中均匀扩散到云母中; 使用水来降低混合物的温度以形成碱性溶液; 将粉状云母与碱性溶液分离,得到固体云母; 通过用冷水稀释的酸溶液中和固体云母附着的过量碱性化合物,并且在将云母的pH调节至7.0之后,云母抗膨胀; 再通过加入水稀释酸溶液,并从稀酸溶液中分离出固体云母,得到生产 - 抗膨胀云母。