    • 5. 发明申请
    • AN OPTICAL GLASS AND OPTICAL ELEMENT
    • 光学玻璃和光学元件
    • US20140287906A1
    • 2014-09-25
    • US14349600
    • 2012-09-18
    • CDGM GLASS CO., LTD
    • Bo Kuang
    • C03C3/068
    • C03C3/068C03C3/155
    • The invention provides an optical glass, which includes 6 wt % to 10 wt % of B2O3; 10 wt % to 15% of B2O3 and SiO2, wherein the content of B2O3 is more than that of SiO2; 27 wt % to 32 wt % of La2O3; 0 wt % to 5 wt % of Gd2O3, Y2O3 and Yb2O3, wherein the content of Gd2O3 is 0 wt % to 3 wt %; more than 19 wt % but less than 25 wt % of TiO2; more than 8 wt % but less than 15 wt % of Nb2O5; 0.5 wt % to 5 wt % of ZnO; 0 wt % to 2 wt % of WO3; 2 wt % to 10 wt % of ZrO2; more than 10 wt % but less than 15 wt % of BaO; 0 wt % to 5 wt % of CaO, SrO and MgO, wherein the content of SrO is 0 wt % to 3 wt %; and 0 wt % to 0.1 wt % of Sb2O3.
    • 本发明提供一种光学玻璃,其包含6重量%至10重量%的B 2 O 3; 10%〜15%的B2O3和SiO2,其中B2O3的含量大于SiO2的含量; 27重量%至32重量%的La 2 O 3; 0重量%〜5重量%的Gd 2 O 3,Y 2 O 3和Yb 2 O 3,其中Gd 2 O 3的含量为0重量%〜3重量% 大于19重量%但小于25重量%的TiO 2; 大于8重量%但小于15重量%的Nb 2 O 5; 0.5重量%〜5重量%的ZnO; 0重量%至2重量%的WO 3; 2重量%〜10重量%的ZrO 2; 大于10重量%但小于15重量%的BaO; 0重量%〜5重量%的CaO,SrO和MgO,其中SrO的含量为0重量%〜3重量% 和0重量%〜0.1重量%的Sb 2 O 3。
    • 6. 发明授权
    • Optical glass and optical element
    • 光学玻璃和光学元件
    • US08835334B2
    • 2014-09-16
    • US13703048
    • 2011-09-12
    • Takahiro MatanoFumio Sato
    • Takahiro MatanoFumio Sato
    • C03C3/064C03C3/14C03C3/066C03C3/15C03C3/145C03C3/068C03C3/155C03C4/02
    • C03C4/02C03C3/064C03C3/066C03C3/068C03C3/14C03C3/145C03C3/15C03C3/155
    • Provided is an optical glass which can satisfy all of the following requirements: (1) it contains no environmentally undesirable components; (2) it can easily achieve a low glass transition point; (3) it has a high refractive index and high dispersion; (4) it can easily provide a glass having a superior visible light transmittance; and (5) it has superior resistance to devitrification during preparation of a preform. The optical glass has a refractive index nd of 2.0 or more, an Abbe's number νd of 20 or less, a glass transition point of 450° C. or below, and a glass composition, in % by mass, of 70 to 90% Bi2O2, 4 to 29.9% B2O2, 0.1 to 10% Li2O+Na2O+K2O, and 0 to 2.5% SiO2+Al2O2 and is substantially free of lead component, arsenic component, F component, TeO2, and GeO2.
    • 提供可以满足以下所有要求的光学玻璃:(1)不含有环境不良成分; (2)可以轻松实现低玻璃化转变点; (3)折射率高,色散高; (4)可以容易地提供具有优异的可见光透射率的玻璃; 和(5)在制备预成型品时具有优异的抗失透性。 光学玻璃的折射率nd为2.0以上,阿贝数n为20以下,玻璃化转变温度为450℃以下,玻璃组合物的质量%为70〜90 4%〜29.9%的B 2 O 2,0.1〜10%的Li 2 O + Na 2 O + K 2 O,0〜2.5%的SiO 2 + Al 2 O 2,并且基本上不含铅成分,砷成分,F成分,TeO 2和GeO 2。
    • 7. 发明申请
    • OPTICAL GLASS FOR MOLD PRESS FORMING
    • 用于模压成型的光学玻璃
    • US20120065051A1
    • 2012-03-15
    • US13320755
    • 2010-06-14
    • Takahiro MatanoFumio SatoYoko Usui
    • Takahiro MatanoFumio SatoYoko Usui
    • C03C3/253C03C3/064C03C3/155C03C3/14
    • C03C4/02C03C3/14C03C3/15C03C3/155C03C3/253
    • The invention provides an optical glass for press molding which can satisfy all of the following requirements: (1) it contains no environmentally undesirable components; (2) it can easily achieve a low glass transition point; (3) it has a high refractive index and high dispersion; (4) it can easily provide a glass having an excellent visible light transmittance; and (5) it has excellent resistance to devitrification during preparation of a preform. The optical glass for press molding has a refractive index nd of 1.925 or more, an Abbe's number νd of 10 to 30, and a glass composition, in % by mass, of 20 to 80% Bi2O3, 10 to 30% B2O3, and 0 to 5.5% GeO2 and is substantially free of lead component, arsenic component, and F component.
    • 本发明提供了一种用于压制成型的光学玻璃,其可以满足以下所有要求:(1)其不含环境不理想的组分; (2)可以轻松实现低玻璃化转变点; (3)折射率高,色散高; (4)可以容易地提供具有优异的可见光透射率的玻璃; 和(5)在制备预成型件时具有优异的耐失透性。 用于压制成形的光学玻璃的折射率nd为1.925以上,阿贝数n为10〜30,玻璃组合物的质量%为20〜80%Bi 2 O 3,10〜30%B 2 O 3, 和0〜5.5%的GeO 2,并且基本上不含铅成分,砷成分和F成分。
    • 10. 发明申请
    • OPTICAL GLASS, PREFORM FOR PRECISION PRESS-MOLDING, OPTICAL ELEMENT, METHODS FOR MANUFACTURING THEREOF, AND IMAGING DEVICE
    • 光学玻璃,用于精密压模的光学元件,其制造方法和成像装置
    • US20100255979A1
    • 2010-10-07
    • US12599405
    • 2009-05-28
    • Yasuhiro Fujiwara
    • Yasuhiro Fujiwara
    • C03C3/155C03B23/00C03C3/15C03C3/068
    • C03C3/155C03B11/00C03C3/068C03C3/15
    • An optical Glass characterized by comprising, denoted as molar percentages: B2O35 to 45 percent; Li2O0 to 3 percent; ZnO10 to 40 percent; La2O35 to 30 percent; Gd2O30 to 20 percent; and at least one from among TiO2, Nb2O5, WO3, and Bi2O3; in that the total content X of Ti, Nb, W, and Bi, denoted as a cation percentage, is 3 to 35 percent; in that the Abbé number v(nu)d and refractive index nd fall within the range delimited by sequentially connecting with straight lines points A, B, C, D and A in FIG. 1; and in that the glass transition temperature Tg satisfies relation (1) below: Tg[° C.]≦655° C.−5×X  (1). An optical Glass characterized by comprising, denoted as molar percentages: B2O55 to 45 percent; SiO20 to 6 percent (excluding 6 percent); Li2O, Na2O, K2O in total0 to 3 percent; ZnO10 to 40 percent; La2O35 to 30 percent; Gd2O30 to 20 percent; and ZrO2, TaO2, TiO2, Nb2O5,12.5 to 20 percent; WO3, and Bi2O3 in total in that the cation ratio of the Ti4+ content relative to the total content of Zr4+, Ta5+, Ti4+, Nb5+, W6+, and Bi3+ is 0.30 or lower; in that the temperature Tp at which a viscosity of 107.2 dPa·s is exhibited is 706° C. or lower; and in that the refractive index nd and the Abbé number v(nu)d satisfy all of relations (I) to (IV) below. 34.0≦vd
    • 一种光学玻璃,其特征在于包括:摩尔百分比:B2O3 5〜45% Li2O 0〜3% ZnO为10〜40% La2O3 5〜30% Gd2O3 0〜20% 和TiO 2,Nb 2 O 5,WO 3和Bi 2 O 3中的至少一种; 因为以阳离子百分比表示的Ti,Nb,W和Bi的总含量X为3〜35%。 因为Abbé数v(nu)d和折射率nd落在通过依次连接图1中的直线点A,B,C,D和A所界定的范围内。 1; 并且玻璃化转变温度Tg满足以下关系式(1):Tg [℃]&lt; 111; 655℃-5×X(1)。 一种光学玻璃,其特征在于包括:摩尔百分比:B2O5 5〜45%; SiO2 0〜6%(不含6%); Li2O,Na2O,K2O总计为0〜3%; ZnO为10〜40% La2O3 5〜30% Gd2O3 0〜20% 和ZrO2,TaO2,TiO2,Nb2O5,12.5〜20%; WO 3和Bi 2 O 3的含量相对于Zr4 +,Ta5 +,Ti4 +,Nb5 +,W6 +和Bi3 +的总含量的Ti 4+的阳离子比为0.30以下; 由于表现出粘度为107.2dPa·s的温度Tp为706℃以下, 并且折射率nd和Abbé数v(nu)d满足以下所有关系(I)至(IV)。 34.0&nlE; vd <40(I)nd≥1.87(II)nd≥2.23-0.01×vd(III)nd&nlE; 2.28-0.01×vd(IV)