    • HEALING AGENT FOR SELF-HEALING CEMENTIOUS MATERIAL
    • 自愈式化疗材料的治疗剂
    • US20160347658A1
    • 2016-12-01
    • US14542404
    • 2014-11-14
    • Technische Universiteit Delft
    • Hendrik Marius JONKERS
    • C04B20/10C04B28/02
    • C04B20/1022C04B20/10C04B20/1029C04B20/12C04B28/02C04B40/0042C04B2103/0001C04B2111/2038C04B24/04C04B24/10
    • The invention provides a process for the production of a cementious material. The process comprises mixing cement starting materials and a particulate healing agent to provide the cementious material. The healing agent comprises coated particles, wherein the coated particles comprise bacterial material and additive. The bacterial material is selected from the group consisting of a bacterium, a lyophilized bacterium and a bacterial spore of a bacterium. The present invention solves these problems, as (substantially leakage-proof) tablets containing the actual healing agent may neither interfere with either the workability of the liquid mixture (“cementious material”) nor negatively affect properties of either mixture or final material (hardened concrete), even when applied in large quantities. During crack formation in cementious based constructions, the particles also crack, and healing agent is released.
    • 本发明提供一种生产胶结材料的方法。 该方法包括混合水泥起始材料和颗粒愈合剂以提供粘结材料。 愈合剂包括涂覆的颗粒,其中涂覆的颗粒包括细菌材料和添加剂。 细菌材料选自细菌,冻干细菌和细菌的细菌孢子。 本发明解决了这些问题,因为含有实际愈合剂的(基本上防漏的)片剂既不会干扰液体混合物(“胶结材料”)的可加工性,也不影响混合物或最终材料(硬化混凝土 ),即使大量应用。 在水泥基结构裂缝形成过程中,颗粒也开裂,释放愈合剂。