    • Modified fiber, methods, and systems
    • 改性纤维,方法和系统
    • US09458297B2
    • 2016-10-04
    • US14320279
    • 2014-06-30
    • WEYERHAEUSER NR COMPANY
    • Charles E. Miller
    • C08J3/24B01J19/24D21C9/00
    • D21H11/20B01J19/2405B01J2219/24C08J3/24C08J3/246C08J2301/02C08J2333/02C08J2433/02D21C9/00D21C9/001D21C9/002D21C9/005
    • Methods of forming crosslinked cellulose include mixing a crosslinking agent with an aqueous mixture of cellulose fibers containing little to no excess water (e.g., solids content of 25-55%), drying the resulting mixture to 85-100% solids, then curing the dried mixture to crosslink the cellulose fibers. Systems include a mixing unit to form, from an aqueous mixture of unbonded cellulose fibers having a solids content of about 25-55% and a crosslinking agent, a substantially homogenous mixture of non-crosslinked, unbonded cellulose fibers and crosslinking agent; a drying unit to dry the substantially homogenous mixture to a consistency of 85-100%; and a curing unit and to cure the crosslinking agent to form dried and cured crosslinked cellulose fibers. Intrafiber crosslinked cellulose pulp fibers produced by such methods and/or systems have a chemical on pulp level of about 2-14% and an AFAQ capacity of at least 12.0 g/g.
    • 形成交联纤维素的方法包括将交联剂与含有少量至无多余水的纤维素纤维(例如,固体含量为25-55%)的水性混合物混合,将所得混合物干燥至85-100%固体,然后固化干燥 混合物以交联纤维素纤维。 系统包括混合单元,用于从固体含量为约25-55%的无粘合纤维素纤维和交联剂的水性混合物形成混合物,基本均匀的非交联,未结合的纤维素纤维和交联剂的混合物; 干燥单元,将基本均匀的混合物干燥至85-100%的稠度; 和固化单元,并固化交联剂以形成干燥和固化的交联纤维素纤维。 通过这些方法和/或系统生产的纤维间交联的纤维素纸浆纤维具有约2-14%的纸浆水平的化学制品和至少12.0g / g的AFAQ容量。