热词
    • 7. 发明申请
    • PROCESS FOR PRODUCING POLYACETAL COPOLYMER
    • 生产聚乙烯醇共聚物的方法
    • US20170073451A1
    • 2017-03-16
    • US15119561
    • 2014-12-10
    • Polyplastics Co., Ltd.
    • Tadahiro HORIGUCHIEiji MASUDA
    • C08G2/06C08G2/28C08G2/10
    • C08G2/06C08G2/04C08G2/10C08G2/28
    • A process for producing a polyacetal copolymer, the process making catalyst deactivation easy and efficient. Trioxane as a major monomer is copolymerized with one or more comonomers that are a cyclic ether and/or cyclic formal having at least one carbon-carbon bond, using a nonvolatile protonic acid as a polymerization catalyst at 100° C. or lower until the conversion reaches 50% and thereafter at a polymerization environment temperature of 115° C. to 140° C. This process includes: a crushing step in which a dry-process crusher is used to obtain a crude polyacetal copolymer crushed to such a degree that when the crude copolymer is screened with a sieve having an opening size of 11.2 mm, 90 parts by weight or more thereof passes therethrough; and a deactivation step in which a basic compound (e) is added to the crude copolymer and the mixture is melt-kneaded to thereby deactivate the polymerization catalyst.
    • 一种生产聚缩醛共聚物的方法,使催化剂失活的方法简单高效。 作为主要单体的三恶烷与一种或多种作为具有至少一个碳 - 碳键的环醚和/或环状缩甲醛的共聚单体共聚,使用非挥发性质子酸作为聚合催化剂,在100℃以下直至转化 达到50%,之后在115℃至140℃的聚合环境温度下进行。该方法包括:破碎步骤,其中使用干法破碎机获得粗聚缩醛共聚物,该聚缩醛共聚物被粉碎至如 粗共聚物用开口尺寸为11.2mm的筛子筛选,其中90重量份以上通过; 以及将碱性化合物(e)加入到粗共聚物中并使混合物熔融捏合以使聚合催化剂失活的失活步骤。
    • 9. 发明授权
    • Process for preparing polyacetal copolymer
    • 制备聚缩醛共聚物的方法
    • US5844059A
    • 1998-12-01
    • US791469
    • 1997-01-27
    • Kaoru YamamotoHiroyuki Kanai
    • Kaoru YamamotoHiroyuki Kanai
    • C08G2/06C08G2/10C08G2/18C08G2/28C08G6/00C08G2/00
    • C08G2/18C08G2/06C08G2/10C08G2/28
    • To prepare a thermally very stable polyacetal copolymer containing a very small amount of unstable parts in a high yield according to a simple process wherein an isopolyacid or an acid salt thereof is used as the polymerization catalyst in the copolymerization of trioxane as the principal monomer with a comonomer copolymerizable therewith, and wherein deactivation of the catalyst can be effected simply without fail through contact with a basic gas after polymerization without the necessity for any washing step. In the preparation of a polyacetal copolymer by the copolymerization of trioxane as the principal monomer with a cyclic ether or cyclic formal having at least one carbon--carbon bond as a comonomer, the copolymerization is effected using an isopolyacid or an acid salt thereof as the polymerization catalyst, followed by contact with a basic gas as a deactivator to deactivate the catalyst, and subsequent heat-melting treatment of the resulting crude polymer intact without washing thereof.
    • 为了制备含有非常少量的不稳定部分的热非常稳定的聚缩醛共聚物,根据简单的方法,其中在三恶烷作为主要单体的共聚合中使用异多酸或其酸盐作为聚合催化剂, 可与其共聚的共聚单体,并且其中催化剂的失活可以通过在聚合后与碱性气体接触而简单地进行,而不需要任何洗涤步骤。 在通过三恶烷作为主要单体与具有至少一个碳 - 碳键作为共聚单体的环状醚或环状缩甲醛进行共聚制备聚缩醛共聚物时,使用等多酸或其酸性盐作为聚合反应进行共聚 催化剂,然后与作为失活剂的碱性气体接触以使催化剂失活,随后对所得粗聚合物进行热熔融处理而不洗涤。