    • 71. 发明授权
    • Thermoplastic polyurethane with reduced tendency to bloom
    • 热塑性聚氨酯具有降低的开花倾向
    • US08790763B2
    • 2014-07-29
    • US12712329
    • 2010-02-25
    • Julius FarkasCharles P. Jacobs
    • Julius FarkasCharles P. Jacobs
    • B32B1/08C08G18/00
    • B29C45/0001B29C45/7207B29C47/0004B29C47/0011B29C47/0021B29C47/0023B29C47/0026B29C47/78B29C47/8805B29K2075/00B29K2995/0026B29K2995/0088B29L2007/00B29L2023/00C08G18/4238C08G18/664C08G18/7671C08G2410/00Y10T428/139
    • The present invention discloses a thermoplastic polyurethane which is comprised of the reaction product of (1) a hydroxyl terminated polyester intermediate, (2) a polyisocyanate, and (3) a glycol chain extender; wherein the hydroxyl terminated polyester intermediate is comprised of repeat units that are derived from 1,3-propylene glycol and a dicarboxylic acid; wherein the hydroxyl terminated polyester intermediate has a number average molecular weight from 500 to 10,000; and wherein the thermoplastic polyurethane includes hard segments that are the reaction product of the polyisocyanate and the glycol chain extender. This thermoplastic polyurethane is unique in that it has a greatly reduced tendency to bloom. This is highly desirable in applications where high clarity is desired because blooming causes articles containing the thermoplastic polyurethane to be hazy or foggy in appearance. Blooming can also reduce the ability of an article made with the thermoplastic polyurethane to be securely bound to another article with an adhesive.
    • 本发明公开了一种热塑性聚氨酯,其由(1)羟基封端的聚酯中间体,(2)多异氰酸酯和(3)乙二醇增链剂的反应产物组成; 其中羟基封端的聚酯中间体由衍生自1,3-丙二醇和二羧酸的重复单元组成; 其中所述羟基封端的聚酯中间体的数均分子量为500至10,000; 并且其中所述热塑性聚氨酯包括作为所述多异氰酸酯和所述乙二醇扩链剂的反应产物的硬链段。 这种热塑性聚氨酯是独特的,因为它具有大大降低的开花倾向。 这在需要高透明度的应用中是非常需要的,因为起霜使得含有热塑性聚氨酯的物品在外观上模糊或有雾。 开花也可以降低用热塑性聚氨酯制成的制品与粘合剂牢固地结合到另一制品上的能力。
    • 72. 发明授权
    • Process for preparing a polyisocyanurate polyurethane material
    • 聚异氰脲酸酯聚氨酯材料的制备方法
    • US08785570B2
    • 2014-07-22
    • US12089831
    • 2006-09-29
    • Gerhard Jozef BleysEric HuygensStijn RoekaertsMarc VandervesseHans Godelieve Guido Verbeke
    • Gerhard Jozef BleysEric HuygensStijn RoekaertsMarc VandervesseHans Godelieve Guido Verbeke
    • C08G18/00C08G18/10C08G18/09C08G18/76C08G18/48
    • C08G18/092C08G18/4837C08G18/7671
    • A process for preparing a polyisocyanurate polyurethane material, which process comprises reacting a polyisocyanate and an isocyanate-reactive composition, wherein the reaction is conducted at an isocyanate index of 1600 to 100,000 and in the presence of a trimerization catalyst, wherein the polyisocyanate comprises a) 75-100% by weight of diphenylmethane diisocyanate comprising at least 40%, preferably at least 60% and most preferably at least 85% by weight of 4,4′-diphenylmethane diisocyanate and/or a variant of said diphenylmethane diisocyanate which variant is liquid at 25° C. and has an NCO value of at least 20% by weight (polyisocyanate a), and b) 25-0% by weight of another polyisocyanate (polyisocyanate b), the amount of polyisocyanate a) and polyisocyanate b) being calculated on the total amount of this polyisocyanate a) and polyisocyanate b), and wherein the isocyanate-reactive composition comprises a) 80-100% by weight of a polyether polyol having an average nominal functionality of 2-6, an average equivalent weight of 1100-5000 and an oxyethylene (EO) content of 65-100% by weight and b) 20-0% by weight of one or more other isocyanate-reactive compounds, the amount of polyol a) and isocyanate-reactive compound b) being calculated on the total amount of this polyol a) and compound b).
    • 一种制备聚异氰脲酸酯聚氨酯材料的方法,该方法包括使多异氰酸酯和异氰酸酯反应性组合物反应,其中反应在异氰酸酯指数为1600至100,000的条件下进行,并且在三聚催化剂存在下进行,其中多异氰酸酯包含a) 75-100重量%的二苯基甲烷二异氰酸酯,其包含至少40重量%,优选至少60重量%,最优选至少85重量%的4,4'-二苯基甲烷二异氰酸酯和/或所述二苯基甲烷二异氰酸酯的变体,其变体是液体 并且具有至少20重量%的NCO值(多异氰酸酯a),和b)25-0重量%的另一多异氰酸酯(多异氰酸酯b),多异氰酸酯a)和多异氰酸酯的量b)为 基于该多异氰酸酯a)和多异氰酸酯b)的总量计算,并且其中异氰酸酯反应性组合物包含a)80-100重量%的具有平均标称功能的聚醚多元醇 2-6,平均当量为1100-5000,氧化乙烯(EO)含量为65-100重量%,b)20-0重量%的一种或多种其它异氰酸酯反应性化合物,其量为 多元醇a)和异氰酸酯反应性化合物b)根据该多元醇a)和化合物b)的总量计算。
    • 78. 发明授权
    • Aqueous urethane dispersants
    • 水性聚氨酯分散剂
    • US08664331B2
    • 2014-03-04
    • US10496389
    • 2002-11-01
    • Stuart Nicholas Richards
    • Stuart Nicholas Richards
    • B41J2/00B41J2/01B41J2/175C08G18/00C08G18/08C08G18/28C08J3/00C08J3/20C08L75/00
    • C08G18/4833B01F17/005C08G18/0823
    • A polyurethane polymer comprising from 35% to 90% (w/w) of a poly (C2-4-alkylene oxide) based on the total weight of the polymer wherein not less than 60% by weight of the poly (C2-4-alkylene oxide) is polyethylene oxide and wherein at least 5% of the poly (C2-4-alkylene oxide) based on the total weight of the polymer is incorporated in lateral chains and which contains 10 to 180 milliequivalents of add groups for each 100 gm polymer when the polyurethane contains from 35 to 45% by weight poly (C2-4-alkylene oxide), e.g. a polymer made by reacting dimethylolpropionic acid, cyclohexane dimethanol, polypropylene glycol (1000), N-methyl pyrrolidone and an α,α-diydroxy polyethylene glycol obtainable from 2,4-toluene diisocyanate, methoxy polyethylene glycol (750) and diethanolamine.
    • 聚氨酯聚合物,其包含基于聚合物总重量的35%至90%(w / w)的聚(C 2-4 - 烯化氧),其中不少于60重量%的聚(C 2-4 - 环氧烷)是聚环氧乙烷,并且其中基于聚合物总重量的至少5%的聚(C 2-4 - 烯化氧)被并入侧链中,并且对于每100克包含10至180毫当量的加成基团 当聚氨酯含有35至45重量%的聚(C 2-4 - 氧化烯)时, 由二羟甲基丙酸,环己烷二甲醇,聚丙二醇(1000),N-甲基吡咯烷酮和由2,4-甲苯二异氰酸酯得到的α,α-二羟基聚乙二醇,甲氧基聚乙二醇(750)和二乙醇胺制成的聚合物。