    • 83. 发明授权
    • Cationic, capped advanced epoxy resin compositions from glycidyl ethers
of oxyalkylated aromatic or cycloaliphatic diols
    • 阳离子封端的先进环氧树脂组合物由烷氧基化芳族或脂环族二醇的缩水甘油醚组成
    • US5360838A
    • 1994-11-01
    • US77835
    • 1993-06-14
    • Kenneth W. AndersonRichard A. Hickner
    • Kenneth W. AndersonRichard A. Hickner
    • C08G59/06C08G59/14C08G59/22C09D5/44C08K3/20C08L63/02
    • C08G59/226C08G59/066C08G59/14C09D5/4434
    • An advanced epoxy cationic resin useful as an electrodeposition coating and having a charge density of from 0.2 to 0.6 milliequivalent of cationic charge per gram of resin is prepared by reacting in the presence of a suitable catalyst (A) a composition comprising (1) at least one diglycidyl ether of (a) an oxyalkylated aromatic diol or (b) an oxyalkylated cycloaliphatic diol or (c) certain oxyalkylated aliphatic diols and (2) at least one diglycidyl ether of a dihydric phenol with (B) at least one dihydric phenol and optionally (C) a monofunctional capping agent.Components (A-1) and (A-2) are employed in quantities such that from 10 to 75 weight percent of the diglycidyl ethers contained in component (A) are contributed by component (A-1), and from 25 to 90 weight percent of such glycidyl ethers are contributed by component (A-2). Components (A) and (B) are employed in such quantities that the resultant epoxy resin has an average epoxide equivalent weight of from 350 to 10,000. The terminal oxirane groups in the thus formed advanced epoxy resin are converted to cationic groups by reacting the resin with a nucleophilic compound and adding an organic acid and water.
    • 可用作电沉积涂层的电荷密度为0.2-0.6毫当量阳离子电荷/克树脂的高级环氧阳离子树脂通过在合适的催化剂(A)存在下反应制备,该组合物包含(1)至少 (a)烷氧基化芳族二醇的一种二缩水甘油醚或(b)烷氧基化脂环族二醇或(c)某些烷氧基化脂族二醇和(2)至少一种二元酚与(B)至少一种二元酚的二缩水甘油醚和 任选地(C)单官能封端剂。 组分(A-1)和(A-2)的用量使得组分(A)中包含的10至75重量%的二缩水甘油醚由组分(A-1)和25至90重量份 这种缩水甘油醚的百分比由组分(A-2)贡献。 组分(A)和(B)的用量使所得环氧树脂的平均环氧当量为350至10,000。 如此形成的先进环氧树脂中的末端环氧乙烷基团通过使树脂与亲核化合物反应并加入有机酸和水而转化为阳离子基团。