    • 2. 发明授权
    • Laminated ceramic capacitor
    • 层压陶瓷电容器
    • US08526164B2
    • 2013-09-03
    • US13039379
    • 2011-03-03
    • Tomoyuki NakamuraTomonori MurakiMakoto MatsudaAkihiro Shiota
    • Tomoyuki NakamuraTomonori MurakiMakoto MatsudaAkihiro Shiota
    • H01G4/06C04B35/00
    • H01G4/06
    • A laminated ceramic capacitor which provides favorable properties and characteristics such as dielectric characteristics, insulation properties, temperature characteristics, and high temperature load characteristics and provides favorable thermal shock resistance, even when dielectric ceramic layers are reduced in layer thickness to increase the number of layers has dielectric ceramic layers containing, as their main constituent, a barium titanate based compound represented by the general formula ABO3 and internal electrodes containing Ni as their main constituent, which are stacked alternately. A crystalline oxide containing at least Mg and Li is present in at least either one of the internal electrodes and the dielectric ceramic layers. The crystalline oxide is preferably present mostly in contact with Ni in the internal electrodes.
    • 一种叠层陶瓷电容器,其具有良好的性能和特性,例如介电特性,绝缘特性,温度特性和高温负载特性,并提供良好的耐热冲击性,即使介电陶瓷层的厚度减小以增加层数, 以作为主要成分的由通式ABO3表示的钛酸钡类化合物和以Ni为主要成分的内部电极交替叠层的介电陶瓷层。 至少包含Mg和Li的结晶氧化物存在于内部电极和电介质陶瓷层中的至少一个中。 结晶氧化物优选主要与内部电极中的Ni接触。
    • 4. 发明申请
    • LAMINATED CERAMIC CAPACITOR
    • 层压陶瓷电容器
    • US20110216472A1
    • 2011-09-08
    • US13039379
    • 2011-03-03
    • Tomoyuki NakamuraTomonori MurakiMakoto MatsudaAkihiro Shiota
    • Tomoyuki NakamuraTomonori MurakiMakoto MatsudaAkihiro Shiota
    • H01G4/06
    • H01G4/06
    • A laminated ceramic capacitor which provides favorable properties and characteristics such as dielectric characteristics, insulation properties, temperature characteristics, and high temperature load characteristics and provides favorable thermal shock resistance, even when dielectric ceramic layers are reduced in layer thickness to increase the number of layers has dielectric ceramic layers containing, as their main constituent, a barium titanate based compound represented by the general formula ABO3 and internal electrodes containing Ni as their main constituent, which are stacked alternately. A crystalline oxide containing at least Mg and Li is present in at least either one of the internal electrodes and the dielectric ceramic layers. The crystalline oxide is preferably present mostly in contact with Ni in the internal electrodes.
    • 一种叠层陶瓷电容器,其具有良好的性能和特性,例如介电特性,绝缘特性,温度特性和高温负载特性,并提供良好的耐热冲击性,即使当介电陶瓷层的层厚度减小以增加层数时 以作为主要成分的由通式ABO3表示的钛酸钡类化合物和以Ni为主要成分的内部电极交替叠层的介电陶瓷层。 至少包含Mg和Li的结晶氧化物存在于内部电极和电介质陶瓷层中的至少一个中。 结晶氧化物优选主要与内部电极中的Ni接触。
    • 9. 发明授权
    • Monolithic ceramic capacitor
    • 单片陶瓷电容器
    • US09245688B2
    • 2016-01-26
    • US13491627
    • 2012-06-08
    • Akihiro Shiota
    • Akihiro Shiota
    • H01G4/06H01G4/30H01G4/012H01G4/12
    • H01G4/30H01G4/012H01G4/12
    • A monolithic ceramic capacitor having a large capacity and high reliability includes a ceramic sintered body including a plurality of stacked ceramic layers, and first and second inner electrodes and alternately disposed inside the ceramic sintered body to be opposed to each other in a stacking direction of the ceramic layers with one of the ceramic layers being interposed between the adjacent first and second inner electrodes. The ceramic sintered body includes a first portion in which the first and second inner electrodes are opposed to each other, and a second portion positioned outside the first portion. A ratio (Ic/Ia) of c-axis peak intensity (Ic) to a-axis peak intensity (Ia) measured with an XRD analysis of the one of the ceramic layers is about 2 or more.
    • 具有大容量和高可靠性的单片陶瓷电容器包括:陶瓷烧结体,其包括多个层叠的陶瓷层;以及第一和第二内部电极,并且交替地设置在陶瓷烧结体的内部,以相对于陶瓷烧结体的层叠方向 其中一个陶瓷层介于相邻的第一和第二内部电极之间的陶瓷层。 陶瓷烧结体包括第一和第二内部电极彼此相对的第一部分和位于第一部分外侧的第二部分。 通过一个陶瓷层的XRD分析测量的c轴峰值强度(Ic)与a轴峰值强度(Ia)的比(Ic / Ia)约为2或更大。