    • 2. 发明授权
    • Hard coat film
    • 硬涂膜
    • US06562440B1
    • 2003-05-13
    • US09675048
    • 2000-09-29
    • Mitsuru TsuchiyaTakahiro Niimi
    • Mitsuru TsuchiyaTakahiro Niimi
    • B32B2714
    • C08J7/04C08J7/045C08J2367/02Y10T428/24802Y10T428/24901Y10T428/24942Y10T428/2495Y10T428/24983Y10T428/25Y10T428/31
    • The present invention relates to a hard coat film used for various types of displays, wherein cracking and peeling of the hard coat layer is prevented, hardness reduction of the hard coat film is suppressed and the pencil hardness of the hard coat film is in the range of 4H-8H. The hard coat film includes a buffer layer (2) with a thickness of 3-50 &mgr;m, formed on at least one side of a plastic base film (1), which has a buffer function against deformation of the hard coat layer in response to deformation of the plastic base film (1), and a hard coat layer (3) with a thickness of 3-15 &mgr;m additionally formed over the buffer layer. The hard coat film (9) is designed so that the pencil hardness of the plastic base film (1), the pencil hardness of the buffer layer and the pencil hardness of the hard coat layer increase in that order.
    • 本发明涉及用于各种显示器的硬涂膜,其中防止硬涂层的破裂和剥离,硬涂膜的硬度降低被抑制,硬涂膜的铅笔硬度处于 的4H-8H。 硬涂膜包括厚度为3-50μm的缓冲层(2),形成在塑料基膜(1)的至少一侧上,其具有缓冲功能,以抵抗硬涂层响应于 在缓冲层上另外形成塑料基膜(1)的变形和厚度为3-15μm的硬涂层(3)。 硬涂膜(9)的设计使得塑料基膜(1)的铅笔硬度,缓冲层的铅笔硬度和硬涂层的铅笔硬度依次增加。
    • 7. 发明授权
    • Hard coat film
    • 硬涂膜
    • US06329041B1
    • 2001-12-11
    • US09251418
    • 1999-02-17
    • Mitsuru TsuchiyaTakahiro Niimi
    • Mitsuru TsuchiyaTakahiro Niimi
    • B32B2714
    • C08J7/04C08J7/045C08J2367/02Y10T428/24802Y10T428/24901Y10T428/24942Y10T428/2495Y10T428/24983Y10T428/25Y10T428/31
    • The present invention relates to a hard coat film used for various types of displays, wherein cracking and peeling of the hard coat layer is prevented, hardness reduction of the hard coat film is suppressed and the pencil hardness of the hard coat film is in the range of 4H-8H. The hard coat film includes a buffer layer (2) with a thickness of 3-50 &mgr;m, formed on at least one side of a plastic base film (1), which has a buffer function against deformation of the hard coat layer in response to deformation of the plastic base film (1), and a hard coat layer (3) with a thickness of 3-15 &mgr;m additionally formed over the buffer layer. The hard coat film (9) is designed so that the pencil hardness of the plastic base film (1), the pencil hardness of the buffer layer and the pencil hardness of the hard coat layer increase in that order.
    • 本发明涉及用于各种显示器的硬涂膜,其中防止硬涂层的破裂和剥离,硬涂膜的硬度降低被抑制,硬涂膜的铅笔硬度处于 的4H-8H。 硬涂膜包括厚度为3-50μm的缓冲层(2),形成在塑料基膜(1)的至少一侧上,该缓冲层具有缓冲功能,以抵抗硬涂层响应于 在缓冲层上另外形成塑料基膜(1)的变形和厚度为3-15μm的硬涂层(3)。 硬涂膜(9)的设计使得塑料基膜(1)的铅笔硬度,缓冲层的铅笔硬度和硬涂层的铅笔硬度依次增加。
    • 9. 发明授权
    • Optical functional materials and process for producing the same
    • 光学功能材料及其制造方法
    • US5909314A
    • 1999-06-01
    • US388257
    • 1995-02-13
    • Motohiro OkaMitsuru TsuchiyaNorinaga NakamuraKiyotaka TakematusYurie OtaHiroko SuzukiNatsuko YamashitaHiroomi Katagiri
    • Motohiro OkaMitsuru TsuchiyaNorinaga NakamuraKiyotaka TakematusYurie OtaHiroko SuzukiNatsuko YamashitaHiroomi Katagiri
    • G02B1/11G02B1/12G02B1/10
    • G02B1/111G02B1/11G02B1/12
    • A antiglare layer 12 having a fine uneven surface is formed directly or through other layer(s) on a transparent substrate film 11, and a layer 13 having a low refractive index, which is lower than the refractive index of the antiglare layer 12, is formed thereon. The refractive index of the antiglare layer 12 is higher than the refractive index of a layer in contact with said antiglare layer 12 on its surface remote from the layer 13 having a low refractive index. An SiO.sub.x film may be used as the layer 13 having a low refractive index. The SiO.sub.x film per se has excellent gas barrier property and antifouling property as an optical functional membrane and is an optical functional material characterized by having excellent moistureproofness, scratch resistance, adhesion to a substrate, transparency, low refractive index, dye deterioration preventive property, and other properties. A layer 13 having a low-refractive index as a surface layer is formed through other layer(s) on a transparent substrate film 11, and at least one of the other layer(s) is a hard coat layer 12 of 0.5 .mu.m or more in thickness, having a high refractive index, composed mainly of a resin. The hard coat layer 12 having a high refractive index is in direct contact with a layer 13 having a low refractive index. The refractive index of the hard coat layer 12 having a high refractive index is higher than the refractive index of a layer in contact with the hard coat layer 12 having a high refractive index on its surface remote from the layer 13 having a low refractive index. For use, the antireflection film is laminated to a polarizing plate or a liquid crystal display device.
    • 直接或透过其他层形成具有微细凹凸表面的防眩光层12,低折射率低于防眩光层12折射率的层13为 形成在其上。 防眩层12的折射率高于与远离具有低折射率的层13的表面上与所述防眩光层12接触的层的折射率。 可以使用SiO x膜作为低折射率的层13。 SiOx膜本身具有优异的阻气性和防污性,作为光学功能膜,是具有优异的防湿性,耐划伤性,对基材的粘附性,透明性,低折射率,染色劣化防止性的特征的光学功能材料,以及 其他属性。 通过透明基材膜11上的其它层形成作为表层的低折射率层13,其他层中的至少一层为0.5μm的硬涂层12或 厚度更多,折射率高,主要由树脂组成。 具有高折射率的硬涂层12与具有低折射率的层13直接接触。 具有高折射率的硬涂层12的折射率高于在远离具有低折射率的层13的表面上具有高折射率的硬涂层12的层的折射率。 为了使用,将抗反射膜层压到偏振片或液晶显示装置。