    • 1. 发明授权
    • Polymer alloy and production method thereof
    • 聚合物合金及其制备方法
    • US08338547B2
    • 2012-12-25
    • US12680436
    • 2008-09-18
    • Hiroshi TakahashiSadayuki Kobayashi
    • Hiroshi TakahashiSadayuki Kobayashi
    • C08G75/14C08L81/04B29K67/00B29K101/12B29K81/00
    • C08J3/005C08J3/28C08L77/00C08L79/08Y10T428/31786
    • To provide a structure material having excellent mechanical characteristics and a functional material having excellent regularity, provided are a polymer alloy which is composed of at least two components of thermoplastic resins and of which the structure can be controlled finely and evenly dispersed and a production method of the polymer alloy. With respect to a polymer alloy composed of at least two or more components of thermoplastic resins, a precursor (A) of at least one thermoplastic resin among the thermoplastic resin components composing the polymer alloy is chemically reacted in the co-presence of the remaining thermoplastic resin component (B1) and/or a precursor (B2) of the thermoplastic resin component to induce spinodal decomposition, so that it is made possible to obtain a polymer alloy having excellent regularity and of which the structure is finely controllable and the structure is evenly dispersed.
    • 为了提供具有优异机械特性的结构材料和具有优异规则性的功能材料,提供了由热塑性树脂的至少两种组分组成并且其结构可以精细均匀分散的聚合物合金和制备方法 聚合物合金。 对于由至少两种以上的热塑性树脂成分构成的聚合物合金,构成聚合物合金的热塑性树脂成分中的至少一种热塑性树脂的前体(A)在剩余的热塑性树脂的共存下进行化学反应 树脂成分(B1)和/或热塑性树脂成分的前体(B2)引起旋节状分解,使得可以获得具有优异规则性并且其结构精细可控且结构均匀的聚合物合金 分散
    • 2. 发明申请
    • POLYMER ALLOY AND PRODUCTION METHOD THEREOF
    • 聚合物合金及其生产方法
    • US20100216946A1
    • 2010-08-26
    • US12680436
    • 2008-09-18
    • Hiroshi TakahashiSadayuki Kobayashi
    • Hiroshi TakahashiSadayuki Kobayashi
    • C08L77/00C08L81/04C08L33/04
    • C08J3/005C08J3/28C08L77/00C08L79/08Y10T428/31786
    • To provide a structure material having excellent mechanical characteristics and a functional material having excellent regularity, provided are a polymer alloy which is composed of at least two components of thermoplastic resins and of which the structure can be controlled finely and evenly dispersed and a production method of the polymer alloy. With respect to a polymer alloy composed of at least two or more components of thermoplastic resins, a precursor (A) of at least one thermoplastic resin among the thermoplastic resin components composing the polymer alloy is chemically reacted in the co-presence of the remaining thermoplastic resin component (B1) and/or a precursor (B2) of the thermoplastic resin component to induce spinodal decomposition, so that it is made possible to obtain a polymer alloy having excellent regularity and of which the structure is finely controllable and the structure is evenly dispersed.
    • 为了提供具有优异机械特性的结构材料和具有优异规则性的功能材料,提供了由热塑性树脂的至少两种组分组成并且其结构可以精细均匀分散的聚合物合金和制备方法 聚合物合金。 对于由至少两种以上的热塑性树脂成分构成的聚合物合金,构成聚合物合金的热塑性树脂成分中的至少一种热塑性树脂的前体(A)在剩余的热塑性树脂的共存下进行化学反应 树脂成分(B1)和/或热塑性树脂成分的前体(B2)引起旋节状分解,使得可以获得具有优异规则性并且其结构精细可控且结构均匀的聚合物合金 分散
    • 10. 发明授权
    • Polymer alloy
    • 聚合物合金
    • US07462672B2
    • 2008-12-09
    • US11802762
    • 2007-05-24
    • Sadayuki KobayashiJiro Kumaki
    • Sadayuki KobayashiJiro Kumaki
    • C08L67/02C08L81/04
    • C08L67/02C08J3/005C08L69/00C08L81/02C08L2666/18
    • A polymer alloy of polyphenylene sulfide resin and a polyester resin with polyethylene terephthalate as a main component, and forming a co-continuous structure with a wavelength of concentration fluctuation of 0.001 to 1 μm or a dispersed structure with a distance between particles of to 1 μm. The co-continuous structure or dispersed structure of the polymer alloy is formed by the phase separation caused by spinodal decomposition. The polymer alloy is miscible when the shear rate is kept in a range from 100 to 10000 sec−1, and is separated into phases under no shear flow. The polymer alloy of this invention can provide a molded article, film, fibers and the like respectively with excellent mechanical properties at high productivity.
    • 聚苯硫醚树脂和聚对苯二甲酸乙二醇酯作为主要成分的聚酯树脂的聚合物合金,形成浓度波动为0.001〜1μm的共连续结构体或粒径为1μm的分散结构体 。 聚合物合金的共连续结构或分散结构通过由旋节分解引起的相分离形成。 当剪切速率保持在100至10000秒-1的范围内时,聚合物合金是可混溶的,并且在无剪切流动下分离成相。 本发明的聚合物合金可以分别以高生产率提供优异的机械性能的模塑制品,薄膜,纤维等。