    • 4. 发明授权
    • Meltblown method for producing nonwoven fabrics with hygroscopic metastatic feature
    • 用于生产具有吸湿转移特征的非织造织物的熔喷方法
    • US09573308B2
    • 2017-02-21
    • US14644589
    • 2015-03-11
    • Acelon Chemicals and Fiber Corporation
    • Wen-Tung ChouMing-Yi LaiKun-Shan HuangHsiao-Chi Tsai
    • D01F1/10D04H3/013D04H3/105B29C47/00B29C47/36B29C47/92B29K79/00B29L7/00B29L9/00
    • B29C47/0021B29C47/0014B29C47/364B29C47/367B29C47/92B29C2947/92704B29K2079/08B29L2007/008B29L2009/00
    • A meltblown method for producing nonwoven fabrics with hygroscopic metastatic feature. Firstly, fuse prepared bio-polyamide 6,10 into a melt, then extrude, and blow the melt out spinnerets to form natural bio-polyamide 6,10 filaments laid onto a conveyer to form a substrate fibrous web. Secondly, blend and dissolve prepared pulp by putting N-methylmorpholine N-oxide (NMMO) dissolving solvent, and dehydrate it to form dope, then extrude and blow the dope out spinnerets to form natural cellulose filaments laid up over existing fibrous web of bio-polyamide 6,10 on the conveyer so that a fibrous composite of the bio-polyamide 6,10 and natural cellulose in overlaid lamination is formed thereon. Finally, coagulate and regenerate the fibrous composite of the bio-polyamide 6,10 and natural cellulose by means of ejecting mist aerosol of water, and convert it into nonwoven fabric with hygroscopic metastatic feature by orderly applying post treatments of hydro-entangled needle punching, drying, winding-up processes.
    • 一种用于生产具有吸湿转移特征的无纺织物的熔喷方法。 首先,将制备的生物聚酰胺6,10熔合成熔体,然后挤出,并将熔体吹出喷丝头以形成铺在输送机上的天然生物聚酰胺6,10丝,以形成基材纤维网。 其次,通过将N-甲基吗啉N-氧化物(NMMO)溶解溶剂混合并溶解制备的纸浆,并将其脱水形成纺丝原液,然后将纺丝液挤出并吹出喷丝头,形成天然纤维素细丝, 聚酰胺6,10在输送机上,使得在其上形成叠层层叠的生物聚酰胺6,10和天然纤维素的纤维复合材料。 最后,通过喷雾气雾剂将生物聚酰胺6,10和天然纤维素的纤维复合物凝结再生,并通过有序应用水缠结针刺的后处理将其转变成具有吸湿转移特征的无纺织物, 干燥,清理过程。
    • 5. 发明授权
    • Rubber extrusion device
    • 橡胶挤出装置
    • US09566737B2
    • 2017-02-14
    • US14420703
    • 2013-08-30
    • SUMITOMO RUBBER INDUSTRIES LTD.
    • Hiroyuki Onimatsu
    • B29C47/36B29K21/00B29L31/00
    • B29C47/36B29B7/428B29B7/582B29B7/7495B29C47/0004B29C47/08B29C47/364B29C47/367B29C47/38B29C47/665B29D30/60B29K2021/00B29L2031/001
    • The present invention can save space. A rubber extrusion device (1) containing a rubber extruder (2) for kneading rubber and extruding same from a discharge port (7), and a gear pump (3) connected to the discharge port (7) of the rubber extruder (2). The rubber extruder (2) has a cylinder part (4), which houses a rubber extrusion screw (5), above the floor surface on which the rubber extruder (2) is placed. The gear pump (3) contains an electric motor (8), a decelerator (9) linked to the electric motor (8), and a gear pump main body (10) linked to the decelerator (9). A pair of gears (11) which meshes with one another is installed in the gear pump main body (10). The electric motor (8) and the decelerator (9) are disposed in a space below the gear pump main body (10) or the cylinder part (4). Moreover, the output shaft (9b) of the decelerator and one of the gears (11) are linked by means of a wrapping transmission means.
    • 本发明可以节省空间。 一种橡胶挤出装置(1),其包含用于捏合橡胶并从排出口(7)挤出的橡胶挤出机(2)和连接到橡胶挤出机(2)的排出口(7)的齿轮泵(3) 。 橡胶挤出机(2)具有在橡胶挤出机(2)所在的地板表面上方容纳橡胶挤出螺杆(5)的圆筒部分(4)。 齿轮泵(3)包括电动机(8),连接到电动机(8)的减速器(9)和与减速器(9)连接的齿轮泵主体(10)。 一对齿轮(11)彼此啮合安装在齿轮泵主体(10)中。 电动机(8)和减速器(9)设置在齿轮泵主体(10)或气缸部(4)的下方的空间内。 此外,减速器的输出轴(9b)和齿轮(11)中的一个通过包装传动装置连接。
    • 9. 发明申请
    • Spunbond method for producing non-woven fabric with deodorant feature from bamboo cellulose
    • 用于生产竹纤维素除臭功能的无纺织物的纺粘方法
    • US20160214302A1
    • 2016-07-28
    • US14666649
    • 2015-03-24
    • Acelon Chemicals and Fiber Corporation
    • Wen-Tung CHOUMing-Yi LAIKun-Shan HUANG
    • B29C47/00
    • B29C47/0004B29C47/0014B29C47/367B29K2001/00B29K2001/08B29K2311/10B29L2007/002D01D1/02D01F1/10D01F2/00
    • A spunbond method for producing non-woven fabric with deodorant feature from bamboo cellulose comprises following process steps. Prepare bamboo pulp mixture by blending bamboo pulp and coffee residue in proper mixing ratio. Put N-methylmorpholine N-oxide (NMMO) as solvent and 1, 3-phenylene-bis 2-oxazoline (BOX) as stabilizer into prepared bamboo pulp mixture to form dope. Via spunbond method, orderly perform extruding, spinning, quenching and pre-drawing process to convert the dope into bamboo filaments of fibrous strand. Orderly process coagulation, regeneration and post-draw to the bamboo filaments of fibrous strand to transform them into uniform fine bamboo cellulose filaments. Bond and lay these bamboo filaments of fibrous strand on a belt collector to form a webbed nonwoven. After post treatments of water rinsing, hydro-entangled needle punching and drying have been orderly applied, then a resultant nonwoven fabric in continuous filament of bamboo cellulose with deodorant feature is produced from the webbed nonwoven.
    • 用于生产竹纤维除臭特性的无纺织物的纺粘方法包括以下步骤。 通过以适当的混合比混合竹浆和咖啡残渣来制备竹浆混合物。 将N-甲基吗啉N-氧化物(NMMO)作为溶剂和1,3-亚苯基 - 双2-恶唑啉(BOX)作为稳定剂加入到制备的竹浆混合物中以形成涂料。 通过纺粘法,有序地进行挤出,纺丝,淬火和预拉伸过程,将纺丝原液转化成纤维束竹丝。 有序的处理凝固,再生和后拉丝到纤维束的竹丝上,将其转变成均匀的细竹纤维素丝。 粘合并将这些纤维束的竹丝放在带状收集器上以形成网状非织造布。 经过水洗后处理后,水刺针刺干燥得到有序的施用,然后由网状无纺布制成竹纤维素连续长纤维带除臭特征的非织造织物。