    • METHOD FOR PRODUCING POLYESTER FIBERS, POLYESTER FIBERS, YARNS AND TEXTILES
    • 生产聚酯纤维,聚酯纤维,纱线和纺织品的方法
    • US20150252494A1
    • 2015-09-10
    • US14631478
    • 2015-02-25
    • SHINKONG SYNTHETIC FIBERS CORPORATION
    • YI-JEN TUKUO-CHUNG WUYUAN-CHEN LIAO
    • D01F8/14C08L67/02
    • D01F8/14C08L67/02D01F6/92Y10T428/249921Y10T428/2973C08L67/00
    • The present invention provides a method for producing polyester fibers which improves the defects that polyester fibers and the textiles thereof cannot be easily dyed. In such method, fibers could be dyed by using dispersed dyes at ambient pressure and a temperature of 100° C. or less without adding carrying agents, and have good dyeability, high dyeing deepness and excellent color fastness. The textiles thereof have excellent dyeing retention. In the said method for producing fibers which could be easily dyed at low temperature, a composition consisting of 99.9 to 60% by weight of a first polyester component with a glass transition temperature (Tg) of greater than 20° C. to 100° C. and 0.1 to 40% by weight of a second polyester component with a glass transition temperature (Tg) of 20° C. to −50° C. is melted and spun to such polyester fibers.
    • 本发明提供一种改善聚酯纤维及其纺织品难以染色的缺点的聚酯纤维的制造方法。 在这种方法中,纤维可以在环境压力和温度为100℃以下的分散染料中染色,而不添加载体,并且具有良好的可染性,高染色深度和优异的色牢度。 其纺织品具有优异的染色保留性。 在所述的生产低温易染色纤维的方法中,由99.9-60%重量的玻璃化转变温度(Tg)大于20℃至100℃的第一聚酯组分组成的组合物 和0.1至40重量%的玻璃化转变温度(Tg)为20℃至-50℃的第二聚酯组分熔融并纺丝至这种聚酯纤维。